Many years ago I ran across a paper that said you're OK as long as the ratio of part weight to total land area is less than 0.81 g/mm^2. This was in the SnPb days, but since the surface tension of SAC is higher than SnPb the rule should still be valid. The paper is long gone so I can't give a citation. Let's say the pad diameter for your BGA is 0.3 mm. The ratio works out to 0.039 g/mm^2 so you'll be fine. I can't imagine a BGA that wouldn't have enough surface tension to hang on during upside down reflow.
Scott Post
Staff Manufacturing Engineer
P.O.U. 0000-001E-0CTC
2151 E. Lincoln Road
Kokomo, Indiana 46904-9005
765-451-2983 (Phone)
765-451-0287 (FAX)
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leif Erik Laerum
Sent: Friday, April 01, 2011 2:11 PM
To: [log in to unmask]
Subject: [TN] BGA on Solder Side
Technetters,
We are faced with a design that puts 2 BGAs on the solder side of a
board. It will therefore go through reflow on the bottom when building
the other side. The BGA is 19 x 19 mm 484 balls .8mm pitch. Av Weight
1.3302 g. This is a lead free design. I seem to have seen a paper on
the subject discussed on technet, but the archives do not work for me
right now.
We have done thousands of boards with BGAs on both sides, but always
small ones with max ball count at 84. We have never one this size. Any
experiences out there that you can share? Do's and don'ts? I can tack
the corners of the BGA with SMT adhesive, but I would rather not if I
can avoid it.
--
Leif Erik Laerum
CONFIDENTIALITY NOTICE: This email and any attachments are Texas Memory Systems' proprietary material for the exclusive and confidential use of the intended recipient. If you are not the intended recipient, please do not read, distribute or take action in reliance upon this message. Any unauthorized disclosure is prohibited. If you have received this in error, please notify us immediately by return email and promptly delete all copies of this message and its attachments from your computer system.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
**************************************************************************************** Note: If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you. ****************************************************************************************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|