Yes, should have stated that, ENIG finish. That is why they ended up looking pinkish, was the gold showing through the white. Before reflow they were white, after reflow, pinkish. The vendor changed their mask, and we still order them in ENIG, but they stay white after reflow
Lenny Carter
Design Engineer
ERG, Inc.
ph:(607) 754-9187 x3063
www.ergpower.com<http://www.ergpower.com>
www.erglighting.com<http://www.erglighting.com>
_____
From: Paul Edwards [mailto:[log in to unmask]]
Sent: Tuesday, April 26, 2011 4:48 PM
To: [log in to unmask]; [log in to unmask]
Subject: RE: [TN] White solder mask discoloration
Lenny,
Did you use ENIG finish on the pads for the "pinkish" PCB run?
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lenny Carter
Sent: Tuesday, April 26, 2011 1:35 PM
To: [log in to unmask]
Subject: Re: [TN] White solder mask discoloration
We had a couple batches of aluminum clad pcbs for Led lighting that turned
"pinkish" after reflow.
Discussions with the pcb vendor revealed a potential problem with gloss
white mask product the were using. They sampled us the same pcbs using
another white gloss mask, which we ran using the same processes and reflow
profile, and didn't have the problem. The pcb vendor has changed their
white mask recipe as a result, and we have not seen it since.
Lenny Carter
Design Engineer
ERG, Inc.
ph:(607) 754-9187 x3063
www.ergpower.com<http://www.ergpower.com>
www.erglighting.com<http://www.erglighting.com>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jean-Francois
Bissonnette
Sent: Tuesday, April 26, 2011 4:23 PM
To: [log in to unmask]
Subject: Re: [TN] White solder mask discoloration
Hello again,
Just realized that I forgot an important detail. It is in fact metal core
(Al). Thank you all for your answers. Still investigating the problem, I
will give feedback as soon as we pinpoint the problem...
JF
-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de Dennis Fritz
Envoyé : 25 avril 2011 14:50
À : [log in to unmask]
Objet : Re: [TN] White solder mask discoloration
Most recently, I had seen white solder mask on boards (metal core?) going to
the LED lighting industry (reflectors). I understand the IPC effort on
boards for LED lighting was being centered on the China office. I have
copied David Bergman of IPC on this response, as he may provide links to all
kinds of technology for white mask.
-----Original Message-----
From: Jean-Francois Bissonnette <[log in to unmask]>
To: TechNet <[log in to unmask]>
Sent: Fri, Apr 22, 2011 9:19 am
Subject: [TN] White solder mask discoloration
Hi Technetters,
Does anyone have experience with white solder mask? Any chances of success
assing these through reflow without discoloration?
We had a bunch of them sent to our CM and they all came back with a yellow
o brown discoloration. I believe there are different types of solder masks
ut there but is there some standard regarding their capacity to resist
eat? The process used it RoHS.
Thanks in advance!
Jean-François Bissonnette
_____________________________________________________________________
his email has been scanned by the MessageLabs Email Security System.
or more information please contact helpdesk at x2960 or [log in to unmask]
_____________________________________________________________________
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 16.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
or additional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
_____
size=2 width="100%" align=center>
This email and any attachments thereto may contain private, confidential, and privileged material for the sole use of the intended recipient. Any review, copying, or distribution of this email (or any attachments thereto) by others is strictly prohibited. If you are not the intended recipient, please contact [log in to unmask]<mailto:[log in to unmask]> immediately and permanently delete the original and any copies of this email and any attachments thereto.
_____
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|