TECHNET Archives

April 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Amol Kane <[log in to unmask]>
Date:
Tue, 19 Apr 2011 10:14:32 -0400
Reply-To:
Message-ID:
Content-Transfer-Encoding:
7bit
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
<C23267C3AF7B4842B685FC757EE8A7B8493A52D244@catvesexch01>
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (115 lines)
Hi,

 Out at APEX last week there was a paper about paste release from different
materials. I was surprised at the results. The Ni based materials had some
issues  but try to get the paper. 

Paper and Speaker:

Quantitative Evaluation of New Smt Stencil Materials       Chrys Shea, Shea
Engineering Services  

Bob Kondner

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
Sent: Tuesday, April 19, 2011 9:10 AM
To: [log in to unmask]
Subject: Re: [TN] Stencil Thickness

With a 6 mil and no reduction, you end up with area ratio of 0.69, which is
very close to the critical value of 0.66. I am assuming you will need to do
a reduction on the aperture size which put you under 0.66. you will lose
paste release repeatability below 0.66. You could go with a 5 mil step on
that part, or even 4 mils if the paste volume is sufficient for soldering.
Assuming a 2 mil reduction, your area ratio would be 0.7 with 5 mils (0.87
with 4 mils), which is still above the 0.66 threshold for laser cut
stainless. Also ask if the stencil house can use a Ni based alloy or newer
finer grain steel which gives smoother aperture walls as compared to
standard stainless, thereby improving release.


Amol Kane | Process Engineer
Catalyst Manufacturing Services, Inc.
941 Route 38, Owego NY 13827
Phone: (607) 687-7669 Extn 349 | Website: www.catalystems.com


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jean-Francois
Bissonnette
Sent: Tuesday, April 19, 2011 8:55 AM
To: [log in to unmask]
Subject: [TN] Stencil Thickness

Hello Technetters,

 

We have to order a stencil and I'm not too sure what to do in this
situation.  I use IPC-7525A for selecting the stencil thickness.  While 99%+
of the components are way within the Laser Range, 6mil thickness, there is a
component which leads are 11mil x 34mil.  In the 6mil thickness chart, this
falls in the electroform range.  What I'm a risking if I still select laser
cut, 6 mil thickness?  What would you guys suggest?

 

Thanks to all!

 

JF



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives For additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives For additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2