Hi folks - Here is the Friday Element Quiz Question:
The Question:
This element has two allotropic phases - one is an FCC structure and one
is a HCP structure. This element plays a critical role as an alloying
element in a wide range of metal alloys, cermets and protective
coatings.
This element has only one stable isotope which finds use in food
sterilization and medical radiotherapy. Nearly 6 billion tons of this
element are estimated to exist on the world's seafloor but are not
economically recoverable at today's metal prices. What element is being
described?
Bonus question: In what year was this element's oxide first reduced to
produce the pure element?
The winner of the quiz will put Clumpy to work.
So far Clumpy has:
Week 1 Lamar Young, SCS Coatings
- accomplished nothing (drank lots of coffee)
Week 2 Bev Christian, RIM
- conducted REACH material testing
Week 3 Drew Meyer, Benchmark Electronics Inc.
- Solderability testing and mowed the lawn
Week 4 Ian Fox, Goodrich
- had an epic journey of travel
Week 4 Gary Ferrari, Garrick Global
- unknown
Week 5 Fredrick Miller, Astrolab
- unknown
Week 6 David Nelson, Raytheon
- Was a tackling dummy for Dallas Cowboys
Week 7 Graham Collins, L3 Communications
- Cleaned gutters and painted window trim
Week 8 Bill Noel, ITT Geospatial Systems Division
- unknown
Week 9 Steve Gregory of RD Circuits
- unknown
Week 10 David Bealer of Watchfire Signs
- descaled the in-line wash machine! Ouch!
Week 11 Dick Krug of Sparton Corporation
- assisted with AS9100 quality management systems requirements audit
Week 12 Steve Creswick of Balanced Enterprise Solutions
- Acted as Steve's "go fer" due to a broken leg!
Week 13 Gebhard Neifer, Delphi
- conducted a plasma pre treatment Taguchi DOE for a sealing process
Week 14 Bev Christian, RIM
- assisted with a tin pest investigation/test
Week 15 Bev Christian, RIM
- assisted Bev shoveling snow
Week 16 David Bealer of Waatchfire Signs
- assisted with ????
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
------------------------------------------------------------------------------
This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|