The paper can be found at:
http://www.lpkfusa.com/SMTStencil/whitepapers/index.html
The stencils used were ordered from various vendors without preconditions or
stated purpose.
Regards,
Ahne Oosterhof.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Neifer, Gebhard
Sent: Tuesday, March 22, 2011 23:45
To: [log in to unmask]
Subject: [TN] AW: [TN] AW: [TN] Large Board Printers
Well then let's ask the question in a different way: To all the board shop
guys on the forum:
What do you think is state of the art regarding position accuracy pad to
pad?
Interesting study you performed Ahne, is it possible to get a copy of your
paper/presentation?
TIA, cheers,
Gebhard
-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Ahne Oosterhof
Gesendet: Mittwoch, 23. März 2011 00:23
An: [log in to unmask]
Betreff: Re: [TN] AW: [TN] Large Board Printers
Especially in the newer stencil lasers it is very easy to cut a stencil
after the proper size metal is already glued to the mesh. When cutting the
bare metal sheet before it is mounted in the frame it is exposed to a
different tension than after it is glued to the mesh. The affect of that
tension difference can be noticed especially in stencils for large boards or
panels. (The error due to tension difference can be as much as 65um for a
125um thick stencil.)
Ahne.
PS: my test vehicle was for a board of about 500x350mm with 21,000
apertures.
PPS: Electroformed stencils during manufacture see no stress in the metal!
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Tuesday, March 22, 2011 14:18
To: [log in to unmask]; [log in to unmask]
Subject: Re: [TN] AW: [TN] Large Board Printers
Hi Ahne,
When you say "Stencils cut in a frame" what does that mean?
Aren't most all stencils cut in stainless foil outside of a frame, and then
the foil bonded to the frame around the periphery with a polyester mesh?
Steve
-----Original Message-----
From: Ahne Oosterhof
Sent: Tuesday, March 22, 2011 12:45 PM
To: [log in to unmask]
Subject: Re: [TN] AW: [TN] Large Board Printers
I have been looking for pad-to-pad location accuracy on circuit boards, but
have been unable so far to get clear answers.
I did a study for large board (or panel) aperture-to-aperture location
accuracy for stencils made with different processes and on different laser
systems. The results were quite surprising and have been presented at the
most recent Pan-Pacific conference and are available in the proceedings.
REPORTED CONCLUSION:
For a stencil with optimum aperture positioning accuracy we can conclude
that it is critical to choose the best manufacturing method based on three
main factors: 1. Laser cutting shows better results than photo based
processes, 2. Stencils cut in a frame show very little distortion and 3.
Stencils cut on modern lasers showed significantly better positioning
accuracy.
Would you believe error ranges of more than 175um (7mil)!! And board
pad-to-pad errors only make things worse.
Ahne Oosterhof.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Neifer, Gebhard
Sent: Tuesday, March 22, 2011 08:13
To: [log in to unmask]
Subject: [TN] AW: [TN] Large Board Printers
Good question Steve and I do not have a good answer for you but an
additional question for the forum that relates to the same subject:
Is there an IPC specification that specifies the pad to pad dimension
tolerance. My first guess was that I may find something in IPC-A 600, but no
cigar. Does anybody have an idea whether there is a spec regarding the
location tolerances smt pad to smt pad?
Thanks, cheers,
Gebhard
-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Steve Gregory
Gesendet: Dienstag, 22. März 2011 12:14
An: [log in to unmask]
Betreff: [TN] Large Board Printers
Morning all,
I'm wondering if any of you have had any experience with large board ( 22 X
24" and greater) printers? In particular the Surface Mount Techniques
AUL-2220. How well does it do with small apertures (0201 apertures) and fine
pitch?
Any comments good or bad are welcome. If you would prefer to reply offline,
reply to me directly.
Are there any other players out there that do large board printers?
Thanks!
Steve Gregory
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
****************************************************************************
************ Note: If the reader of this message is not the intended
recipient, or an employee or agent responsible for delivering this message
to the intended recipient, you are hereby notified that any dissemination,
distribution or copying of this communication is strictly prohibited. If you
have received this communication in error, please notify us immediately by
replying to the message and deleting it from your computer. Thank you.
****************************************************************************
************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
****************************************************************************
************ Note: If the reader of this message is not the intended
recipient, or an employee or agent responsible for delivering this message
to the intended recipient, you are hereby notified that any dissemination,
distribution or copying of this communication is strictly prohibited. If you
have received this communication in error, please notify us immediately by
replying to the message and deleting it from your computer. Thank you.
****************************************************************************
************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|