Hi Juan!
Yep, the dross is mostly tin oxides. You will generate more, the more
turbulent the wave is. The few times that I've had a pot get low on tin, I
think it was because we were running a lot of boards with bottomside SMT and
we had the turbulent wave on a lot.
You are also right, just get some pure tin bars and add them in.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Juan T. Marugán
Sent: Thursday, March 10, 2011 3:42 PM
To: [log in to unmask]
Subject: [TN] Solder bath analysis. Sn63Pb37 alloy.
I have a question about the variation of the tin content in the solder
alloy and I'm sure that somebody will explain it me.
Why the tin content decrease more than 1% from the nominal of the
Sn63Pb37 alloy? May it be by the dross...?
I suppose that it will be neccesary to add pure tin. Is it correct?
Thank you for your support. Kind regards.
Juan
Indra Sistemas SA
Spain
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|