UL796 is the fabrication specification. IMO there is no reason to specify a UL compliant board unless it will be used in a UL listed or UL recognized product.
UL is a not for profit company started by insurance companies to help reduce their risk. IMO unless a end product and the board is designed to a UL product spec, a 796 rating doesn't achieve much.
Don Vischulis
Sent from my iPod
On Mar 24, 2011, at 10:52 AM, Jack Olson <[log in to unmask]> wrote:
> Greetings,
>
> We are reviewing our bare board procurement document and Fab Notes, and I'm
> stuck on the part about UL. Reviewing notes from other sources I don't see
> any mention of UL, but I know fabricators have some kind of UL approval
> process (and the 94-Vx rating) and a UL registered logo? (I don't know).
>
> My question is, is the UL involvement primarily for the flammability of the
> MATERIALS they use, or is there more to the story?
>
> More to the point, Is there any reason to specify UL on a fabrication
> drawing (or in a general requirement?)
>
> thanks,
> Jack
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|