Techies
I know that there are solvents with very specific boiling points from 185C to >280C at 5C or 10C increments.
When I was involved in this technology, we used a 220C BP solvent that worked superbly with SAC305 and similar lead-free alloys that gave us a 1C DeltaT.
I would avoid high BP solvents unless your alloy really demands it. Of course part of the problem with most systems is maintaining and controlling the T profile. We did it in our equipment using a sealed chamber. That patented technology is, I believe, now exclusively available out of REHM - with whom I have no association, in case anyone was wondering!
Hope this helps
Graham N
Gen3 Systems, UK
www.gen3systems.com
On 8 Feb 2011, at 20:43, Paul Edwards wrote:
> Have used Alpha WS-809 at 240C if the profile is relatively peaky...
>
> Paul
>
> Paul Edwards
> Process/Quality Engineering
> Surface Art Engineering
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Julie Silk
> Sent: Tuesday, February 08, 2011 12:37 PM
> To: [log in to unmask]
> Subject: Re: [TN] Vapour phase soldering?
>
> For the first, we use VPR at a couple of suppliers, Jabil and Venture, but they
> don't have the capability at all sites.
>
> For the second, the concern is that the standard flux used in tin-lead paste
> typically will not survive 240C. It will burn out and you won't get good joints.
> You can use tin-lead with higher temperature flux.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
> ==============================================================================
>
> This email and any attachments thereto may contain private, confidential, and
> privileged material for the sole use of the intended recipient. Any review, copying,
> or distribution of this email (or any attachments thereto) by others is strictly prohibited.
> If you are not the intended recipient, please contact [log in to unmask]
> immediately and permanently delete the original and any copies of this email and
> any attachments thereto.
>
> ==============================================================================
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|