Well, I don't know about that. I think he was cutting it pretty thin...
Bob L.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Tuesday, February 01, 2011 3:11 PM
To: [log in to unmask]
Subject: Re: [TN] FW: [TN] PCBA Water Wash - Found word(s) remove list in the Text body
Never have I read anything so eloquently put...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey (EHCOE)
Sent: Tuesday, February 01, 2011 11:49 AM
To: [log in to unmask]
Subject: [TN] FW: [TN] PCBA Water Wash - Found word(s) remove list in the Text body
No, but we can air our differences without impinging on the audience's ability to be held in colloidal suspension until flooded with emotion and carried to a purer state of resolve.
Dewey
-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Tuesday, February 01, 2011 12:37 PM
To: TechNet E-Mail Forum; Whittaker, Dewey (EHCOE)
Subject: RE: [TN] PCBA Water Wash
Now, those are sharp words, Dewey! We can't have esteemed members of the Forum cutting each other down like this.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Tuesday, February 01, 2011 1:17 PM
To: [log in to unmask]
Subject: Re: [TN] PCBA Water Wash
So you're saying the use of an air knife just doesn't cut it?
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Tuesday, February 01, 2011 12:02 PM
To: [log in to unmask]
Subject: Re: [TN] PCBA Water Wash
I disagree with Bob...
I have never seen an air knife remove water from all the spaces that can be on a board...
The work fine if you have plenty of clearance between ALL surfaces...
I have seen air knives drive water into spaces where to water's natural surface tension would NOT allow it to go...
When the water evaporates, if it evaporates, it leaves the organo-halogen complexes that supply base materials for dendritic growth...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Tuesday, February 01, 2011 10:23 AM
To: [log in to unmask]
Subject: Re: [TN] PCBA Water Wash
City water is fine if it is removed (air knife) prior to drying.
Run the number on dissolved solids content and calculate or weigh the amount of later left on the board. With a simple blow off you will find the remaining ionic content is very tiny.
Get ionic contamination tests done. City or DI that test results are the important issue.
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Forrester, Michael (H
USA)
Sent: Tuesday, February 01, 2011 12:08 PM
To: [log in to unmask]
Subject: [TN] PCBA Water Wash
I have three questions I hope someone can help me with:
1) We have a vendor that uses "city water" directly into their SMT PCA washer. I believe DI water is industry standard.
Does anyone know if it is documented anywhere? Spec?
2) We had an issue where there was Chlorine contamination and gold dendrites found inside some standard gull-wing 6 pin SMT ICs.
This issue seems to be batch related. The chip manufacturer claims that chlorine is never used in their process. Should the SMT
process expect to handle the possibility that the wash solution may get into a part? The PCA vendor uses unfiltered "city water",
with no cleaner, in the wash process and does a ROSE test on one board of each lot. Since the ROSE test passes, the PCA vendor
is blaming the part manufacturer for having "leaky" parts, since the thinking is the wash is getting into the part and trapped.
3) One issue I have is the water pressure in the wash is 80-100 psi.
I think this is too strong, and should be half of that? You want to
flood the board with water, not hit the board and bounce off?
Thank you in advance.
Best Regards,
Michael Forrester
Sr. Product Engineer
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
========================================================================
======
This email and any attachments thereto may contain private, confidential, and privileged material for the sole use of the intended recipient. Any review, copying, or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact
[log in to unmask]
immediately and permanently delete the original and any copies of this email and any attachments thereto.
========================================================================
======
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
==============================================================================
This email and any attachments thereto may contain private, confidential, and privileged material for the sole use of the intended recipient. Any review, copying, or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and any attachments thereto.
==============================================================================
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|