I think we have to divide it to two:
1. Acceptance from the PCBs shopes - Stains is not acceptable
2. Stains of PCBs after few months in stock - may be acceptable
Reuven
On Wed, Feb 9, 2011 at 4:10 PM, Jack Olson <[log in to unmask]> wrote:
> Good question.... and when looking at an actual board, how is one to
> determine
> visually if we are looking at "staining" or "oxidation/corrosion"?
> Inquiring minds
> want to know.
> (many would say that even oxidized boards are solderable and acceptable.
> right? I think I just read that somewhere...)
>
> Jack
>
> .
> On Tue, 8 Feb 2011 09:20:44 -0500, Glidden, Kevin
> <[log in to unmask]> wrote:
>
> >Morning everyone,
> >I have a question on IPC-4553, specifically, section 3.1 "Visual", and
> specifically regarding staining of immersion silver. The text states "The
> coverage shall be complete and the finish shall be uniform on the surface
> to be
> plated (see Figures 3-1 through 3-5 for properties visually identified with
> IAg
> plated surfaces)" Figure 3-1 shows 'Example of Uniform Plating", with no
> staining. Figures 3-2 through 3-5 show staining. Is this to imply
> (without text
> to support) that any staining of immersion silver is determined to be non-
> uniform and therefore a defect?
> >Thanks.
> >
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|