Hi Cedric,
to solder such components nearly void free I suggest to use a vacuum vapour phase soldering system.
On standard PCBs we run automotive products with low void paste, which is solder paste with less flux, through reflow. The paste reduce the void rate about 10%, additional nitrogen (oxygen less than 100ppm during lead free reflow) can reduce by additional 10% to nearly 5% void rate.
Best regards,
Torsten
i.A. Dipl.Ing.(FH)Torsten Hagge
tech. projectmanager
Kristronics GmbH
Gewerbegrund 5 - 9
24955 Harrislee
Tel.: +49 461 7741 624
Fax: +49 461 7741 642
[log in to unmask]
www.kristronics.de
Gerichtsstand Flensburg, Handelsregister: HRB 1433 FL
Geschäftsführer Dipl.-Ing. oec. Thormod Ohm
Ust-Id-Nr. DE 811182059
Bankverbindung: Deutsche Bank AG Flensburg, Konto-Nr. 4216610, BLZ 21570011
IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215
-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Cedric ORAIN
Gesendet: Donnerstag, 17. Februar 2011 15:26
An: [log in to unmask]
Betreff: [TN] Voids issue on Aluminium base plate
Dear Technetters,
We have to solder a RF power transistor onto an aluminium base plate and we
are facing with a very challenging issue.
We encountered a high voids rate (>30% or 40%) underneath the component body
(which is about 35x10mm). This is not acceptable for this application.
The component is Nickel/gold plated whereas the aluminium baseplate is
plated with Nickel and Silver and then cleaned with solvent.
We tried to change/adapt:
- soak time of the profile,
- 2 difference solder pastes (SAC305),
- change the screen design and thickness
Finally none of these parameters looks to have significant effect on voids
rate. We are now wondering if the solderability of the Ni/Ag plating is good
enough and even if it is convenient for that purpose.
Is somebody could give us advises? How to enhanced NiAg plating
solderability (acid ?!, ...)? Which flux could help to compensate the poor
wettability? Which kind of plating would be preferable? ...
Thanks and regards,
Cedric
-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de Douglas Pauls
Envoyé : jeudi 17 février 2011 14:07
À : [log in to unmask]
Objet : Re: [TN] Electrical Clearance as stated in IPC standards
Good morning Wee Mei,
IPC-T-50, the IPC "dictionary", lists the following:
Electrical Clearance: The shortest distance between two conductors, which
includes traces, terminals and structures, measured through the air.
IPC-T-50 does not contain terms for Clumpy, Trucklett, or Bobby
Dazzler.....
Doug Pauls
Lum Wee Mei <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/16/2011 11:26 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Lum Wee Mei <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Electrical Clearance as stated in IPC standards
Dear All,
Until now, I am still very curious about this term "electrical clearance"
that is used on the IPC standards. Very often, the standard will says
something like "it is acceptable as long as it meets the electrical
clearance". As I did not have the IPC standards with me when I right this,
allow me to use a scenario to illustrate my query :
A digital PCB has some pockets of power and ground area fills with minimum
trace width/clearance of say 6mil/6mil (0.15mm/0.15mm) and power trace
width of 50mil. During bare board inspection (Class 3 requirement), one of
the power trace that run along side of the ground fill, has an excessive
copper protrusion that reduce the physical conductor to conductor
clearance by 60%. Based on the IPC-A-600, it has violate the conductor to
conductor clearance. However, the argument kick-in that it is not a
violation and can be acceptable because the remaining clearance of 40% is
much larger than the electrical clearance stated in IPC-2221 for that
application. Now, how should this be resolved?
Thanks and Regards,
~ Wee Mei ~
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|