From my viewpoint for an internal cap, a thickness or void criteria would not be applicable.
Mike Hill
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Monarchio, James
Sent: Wednesday, February 09, 2011 5:10 PM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] buried cap thickness
Also the fill material may be the resin from lamination, I which case
the via could not be cap plated internally.
Jim
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Jose A
Rios
Sent: Wednesday, February 09, 2011 4:57 PM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] buried cap thickness
unless the design specifically calls out buried caps, we tend to not cap
plate internals.
a generic note like what you cite below "fill, planarize, cap" we tend
to
only apply it to externals.
Joey Rios
PWB & Process Quality Eng'r
Endicott Interconnect Technologies
1093 Clark St.
Endicott, NY 13760
Office: 607-755-5896
Chris Mahanna <[log in to unmask]>
Sent by: IPC-600-6012 <[log in to unmask]>
02/09/2011 04:38 PM
Please respond to
"(Combined Forum of D-33a and 7-31a Subcommittees)"
<[log in to unmask]>
To
[log in to unmask]
cc
Subject
[IPC-600-6012] buried cap thickness
I assume that we purposely did not include a caveat for buried cap
thickness in 6012C?
My particular interest is the case where the design predates 6012C and
gives no more specifics than: "fill, planarize and cap"
Thanks
Chris
Chris Mahanna
President, Technical Manager
Robisan Laboratory Inc.
6502 E. 21st Street
Indianapolis, Indiana 46219
317-353-6249
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
NOTICE: This email message is for the sole use of the intended recipient(s) and may contain confidential and privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply email and destroy all copies of the original message.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|