I would have to agree with Keith.
Pb has been around forever (at least since roman times) and was mined by
iteslf, not as a byproduct
Gallium is mines as a byproduct of Zinc mining. Originally it was left
in the waste and piled high in landfills, but recently has begun to be
recovered for its own sake.
mark
mark
Mark Woolley |PTRL Laboratory | Avaya | 1300 West 120th Ave |
Westminster, CO 80234 USA |
Voice (Lab): (303) 538-2166 | email: [log in to unmask] |
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Keith Calhoun
Sent: Friday, January 28, 2011 6:19 AM
To: [log in to unmask]
Subject: Re: [TN] NTC Friday Element Quiz - the Question
Gallium?
Keith S. Calhoun
Manufacturing Engineering Manager
SoPark Corporation
3300 South Park Avenue
Buffalo, New York 14218
Phone: 716-822-0434 ext. 237
Fax: 716-822-5062
Email: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Friday, January 28, 2011 8:12 AM
To: [log in to unmask]
Subject: [TN] NTC Friday Element Quiz - the Question
Hi folks - Here is the Friday Element Quiz Question:
The Question:
The price of this element has increased by a factor of 6 during the last
2
decades of the 20th Century. The majority of the world production of
this
element comes from fume/dust/slags from Zinc mining. This element is a
superconductor below 3.37K. This element does not oxidize in room
temperature air. Which element is being described?
The winner of this week's quiz will get the exclusive use of Clumpy's
services. Hey Bev - what did Clumpy finally accomplish for you?
So far Clumpy has:
Week 1 Lamar Young, SCS Coatings
- accomplished nothing (drank lots of coffee)
Week 2 Bev Christian, RIM
- conducted REACH material testing
Week 3 Drew Meyer, Benchmark Electronics Inc.
- Solderability testing and mowed the lawn
Week 4 Ian Fox, Goodrich
- had an epic journey of travel
Week 4 Gary Ferrari, Garrick Global
- unknown
Week 5 Fredrick Miller, Astrolab
- unknown
Week 6 David Nelson, Raytheon
- Was a tackling dummy for Dallas Cowboys
Week 7 Graham Collins, L3 Communications
- Cleaned gutters and painted window trim
Week 8 Bill Noel, ITT Geospatial Systems Division
- unknown
Week 9 Steve Gregory of RD Circuits
- unknown
Week 10 David Bealer of Watchfire Signs
- descaled the in-line wash machine! Ouch!
Week 11 Dick Krug of Sparton Corporation
- assisted with AS9100 quality management systems requirements audit
Week 12 Steve Creswick of Balanced Enterprise Solutions
- Acted as Steve's "go fer" due to a broken leg!
Week 13 Gebhard Neifer, Delphi
- conducted a plasma pre treatment Taguchi DOE for a sealing process
Week 14 Bev Christian, RIM
- ????
Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|