TECHNET Archives

January 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Blair Hogg <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Blair Hogg <[log in to unmask]>
Date:
Wed, 26 Jan 2011 13:11:22 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (25 lines)
Do you flux just the pads, or the entire area? It seems like it would be difficult 
to flux only the pads, you would have to screen print flux or something.

Blair

On Wed, 26 Jan 2011 08:56:53 -0600, Stadem, Richard D. <Richard.S@GD-
AIS.COM> wrote:

>Thanks, Mike, another point I forgot to mention.
>When not using solder paste for BGAs, the pads are fluxed with a very fine 
sheen of the proper tacky flux.
>They should be all the same chemistry, never mix them.
>Again, QUALIFY YOUR PROCESS AND MATERIALS.
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2