Hey Bev,
I have the same problem in my home misters (in the HVAC supply). The rule of thumb is that you get much better grain capacity if you exchange Ca and Mg for Na before hitting the DI bed.
The problem is that I'd rather have Ca and Mg sneak through than NaCl.
At the lab, we have a nice little in-line alarm.
I'm sure you do too, somebody just has the set-point too low on that line.
Chris
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Tuesday, January 18, 2011 2:58 PM
To: [log in to unmask]
Subject: Re: [TN] Misting units
Doug,
So why would it be getting past the DI step? Channeling? Used up the DI exchange capacity?
Bev
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, January 18, 2011 2:56 PM
To: TechNet E-Mail Forum; Bev Christian
Subject: Re: [TN] Misting units
Bev,
My guess is that the step prior to DI is a water softening step and the salt is coming from there.
Doug Pauls
Bev Christian <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/18/2011 01:40 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to Bev Christian <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Misting units
TechNetters,
I have another different but related misting unit concern. The water that is supposed to be coming through the misters in my lab is supposed to be DI water, but we are finding, over time, a thin layer of NaCl on equipment situated below the mister and trailing off the farther away one gets. We have definitively IDed the NaCl and we have also used a bottle on a stick to capture the spray from the mister and found NaCl. We are in the process of tracing back the water source to try and find the point of contamination. Has anyone else ever had this problem?
Bev
RIM
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|