Clint:
I suspect strongly that the answer to your question is a definitive "it depends"...
Depends on line and space width, and how "cute" is your "acute".
Smaller the line and space, the more sensitive will be the design to being overly "acute".
Yes, given that the modern PCB fabricator tends to have processing much better organized than days of old, the matter is diminishing, for a given design parameter.
Rudy Sedlak
RD Chemical Company
--- On Tue, 1/11/11, Cote, Clint (GE Intelligent Platforms, US) <[log in to unmask]> wrote:
From: Cote, Clint (GE Intelligent Platforms, US) <[log in to unmask]>
Subject: [TN] Acute Angles
To: [log in to unmask]
Date: Tuesday, January 11, 2011, 9:53 AM
We have a bunch of old references to avoid acute angles when routing
traces. The acute angle would become an acid trap and continue etching
the trace until it reduces it or breaks it completely. Is this still an
issue with modern chemistry and cleaning? Do acute angles present a
long term reliability issue? Are there any studies or evidence that I
can reference?
Thanks,
Clint Cote
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|