I also find this interesting. I am going out on a limb and assuming the rate of copper dissolution is exacerbated, the "force" is actually leaching, not pressure, and the root cause may have been excessive touch-up or rework. Any opinions or observations otherwise?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Monday, January 03, 2011 3:39 PM
To: [log in to unmask]
Subject: Re: [TN] solder joint height values (h) for leadless SMT components?
Dale,
That is interesting. I have a possible dumb question:
You mention copper at 1um or less the copper become deformed such that if
follows the component termination contour.
What is the source of these forces and does this imply the copper is being
torn from the FR4?
Thanks,
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hart, Dale L CTR USAF
AFMC AFRL/RXSA
Sent: Monday, January 03, 2011 3:41 PM
To: [log in to unmask]
Subject: Re: [TN] solder joint height values (h) for leadless SMT
components?
John,
I've been doing failure analysis for the Air Force for nearly 30 years.
I've cross sectioned countless chip resistors and capacitors during this
time. If I find the standoff height of solder under a component termination
greater than 50um it is extremely rare. The average height is between 25 to
40um. Approximately 5 percent of these components have 1um or less. Of
these 1um or less the copper pad underneath the termination is deformed to
the contour of the component termination.
This has also occurred with both iron/nickel and copper "L" shaped gull wing
leads. The manufacturers that populate and reflow these boards tell me that
their stencil was, for example, 7 mils and their paste height was within
their acceptable limits. I have asked if they performed line proofing with a
DPA of representative components at various locations on their panel the
answer is usually no or that is was done so long ago that none of the
present operators remember it being done.
Have I seen failures of solder joints of this pedigree, the answer is yes
but not as many you might expect. It depends on the operational environment
(thermal cycling, shock and vibration). Also these type of solder joints
are very susceptible to cracking if they have been encapsulated.
Dale Hart
UTC Failure Analysis Engineer
dlh
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Nieznanski, John A - GS
Sent: Monday, January 03, 2011 1:24 PM
To: [log in to unmask]
Subject: [TN] solder joint height values (h) for leadless SMT components?
Happy 2011 TechNetters!
The solder joint height parameter "h" is a very sensitive parameter in the
E-W solder fatigue equations per IPC-D-279 and IPC-SM-785, particularly for
leadless components.
For leadless components, it is common to use half the solder stencil height
for "h", in lieu of measured values. So for example, given a 6 mil thick
solder stencil, "h" is often assumed to be 3 mils with some acceptably small
variations, to be quantified and confirmed.
However there are many leadless SMT components that have solder joints that
can not be characterized by a single "h" value. For example, SMT resistors
often have a solder fillet that is between 50% and 100% the thickness of the
component along the outside edge of the terminals and much less under the
terminals. Similary for leadless MELF diodes and castellated LCC packages.
Ideally it would be great to build test boards with all these configurations
to get failure data and correlate these results with DPA measurements of
solder joint cross sections. Are you aware of any published papers that
discuss this type of analysis and/or attempt to derive and correlate an
"effective h" for leadless component types and terminals based on
measurements?
In lieu of any published efforts, does it seems plausible or reasonable to
develop the concept of an "effective h" or "average h" based on several
design and assembly parameters such as solder pad dimensions, wetted
terminal dimensions, solder stencil thickness, component-to-pad
misregistration, etc? Is this just wishful thinking? Alternatively, I
suppose one could make the "weakest link" argument and say that the "minimum
h" is going to dominate the behavior of the solder joint, not the "average
h" or "effective h", since the "minimum h" is where the shear stresses and
strains will concentrate and initiate wearout.
Thanks in advance for any results, comments, thoughts or suggestions that
you can provide............
Regards,
John Nieznanski
________________________________
This e-mail and any files transmitted with it may be proprietary and are
intended solely for the use of the individual or entity to whom they are
addressed. If you have received this e-mail in error please notify the
sender.
Please note that any views or opinions presented in this e-mail are solely
those of the author and do not necessarily represent those of ITT
Corporation. The recipient should check this e-mail and any attachments for
the presence of viruses. ITT accepts no liability for any damage caused by
any virus transmitted by this e-mail.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|