One of the reasons for the space is to assure people are bending the lead via a tool or machine that is holding the lead at the point between the seal of the body and the bend.
Without the IPC standard people would be holding the body and bending the leads, stressing and cracking the seal or breaking the miniscus of capacitors.
John Goulet
MFG/Process Engineer
----- Original Message -----
From: "Jeff Popp" <[log in to unmask]>
To: [log in to unmask]
Sent: Thursday, January 27, 2011 6:58:04 AM
Subject: [TN] IPC 610 - Stress Relief
In the 610 -rev E, clause 7.1.2.2 on page 7-9 deals with lead forming and stress relief. The first criteria mentions lead bends less than 1 lead diameter away from the body being only a process indicator for Class 2. The criteria directly below that calls No stress relief a Defect for Class 2.
It seems a little contradictory to me. If you place a bend less than 1 lead diameter away from the seal, is that really any different than no bend whatsoever? It seems to be splitting hairs and from a practical standpoint, a little difficult to tell the difference.
Any thoughts?
Best Regards,
Jeff
Jeff Popp
Quality Assurance Technician
Compunetix, Inc.
2420 Mosside Blvd.
Monroeville, PA 15146
(412) 858-6184
[log in to unmask]<mailto:[log in to unmask]>
[J-STD-001 Instructor logo 2c]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|