It is the DI water since the resistivity 2-18 megOhms and the lowest reading is .5 meg before you change out the D i's resin and carbon tanks.
I'd use soft water with a 5 micron filter at the source to assure you don't clog the nozzles.
A clear housing will help identify when you should change the filters.
You'll want to put a valve before to shut off the source and one after the filter so the water from higher points don't drain back on you when you change the filter. A directional check valve on the filter's output would work if the verticle pipe is close to the filter.
John Goulet
MFG/Process Engineer
----- Original Message -----
From: "Steve Gregory" <[log in to unmask]>
To: [log in to unmask]
Sent: Wednesday, January 5, 2011 1:52:47 PM
Subject: Re: [TN] Deionized water in misting fans and static electricity
Okay...I'm thinking thunderstorms. But I'm pretty sure this wasn't happening
before we put a DI column in for the water.
We put the humidification in to prevent static, not generate it.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Wednesday, January 05, 2011 1:45 PM
To: [log in to unmask]
Subject: Re: [TN] Deionized water in misting fans and static electricity
Not because of the deionized water as much as the water itself...
Space charge collects on water droplets at emission point and due to
movement... Then the chargeable particulate generates current due to a delta
V in potentials...Think thunderstorms...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, January 05, 2011 10:32 AM
To: [log in to unmask]
Subject: [TN] Deionized water in misting fans and static electricity
This may be an off the wall question but here goes.
We have some misting fans that we use for humidification that we've just
recently put in a deionized water source for.
Now it seems that there's a static charge being generated at the fans that
I've never noticed before. Could it be possible that we're generating a
charge at the fans because of the DI water?
Steve
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
============================================================================
==
This email and any attachments thereto may contain private, confidential,
and
privileged material for the sole use of the intended recipient. Any review,
copying,
or distribution of this email (or any attachments thereto) by others is
strictly prohibited.
If you are not the intended recipient, please contact
[log in to unmask]
immediately and permanently delete the original and any copies of this email
and
any attachments thereto.
============================================================================
==
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|