TECHNET Archives

January 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Date:
Thu, 27 Jan 2011 07:38:38 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Douglas Pauls <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (162 lines)
Precisely.

And, keep in mind that there are many routes to madness: biochemical, 
physical blows, being elected to Congress.....

We use the Mad Hatter and mercury reference whenever we do our Rockwell 
Road Shows, our science and engineering shows for the schools.  A neat 
story.  Also explains the madness in early photo developers which also 
used mercury salts.

And no, Denny, I have not been snorting thermometers, though that might 
explain the blockage in my left nostril...........

Doug Pauls



"Whittaker, Dewey (EHCOE)" <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
01/27/2011 07:33 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] GCMS and Plasma






So you're saying consistant results are like hare today, gone tomorrow.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Charlie Pitarys
Sent: Wednesday, January 26, 2011 3:29 PM
To: [log in to unmask]
Subject: Re: [TN] GCMS and Plasma

GCMS, she is a fickle beast. According to my lab folks here, even when
doping ours with a certain known ingredient she spits back a 70% match.
One response was,  "Be careful as GCMS can lead you down a rabbit hole
real
fast".



CONFIDENTIAL
The content of this message, including any attachments, may contain
privileged and/or confidential information proprietary to Kyzen and is
intended only for the named addressees. If you are not the intended
recipient, you may not disseminate, distribute or copy this email.
Please
notify the sender immediately by email if you have received this email
in
error and delete this email from your system.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Wednesday, January 26, 2011 7:57 AM
To: [log in to unmask]
Subject: [TN] GCMS and Plasma

Thank you all for your insights and comments on my recent questions.
Just
confirms that this forum is one of the best tools in my arsenal.

Doug Pauls
Rockwell Collins

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site 
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2