Inge,
I feel your pain. I had purchased a more expensive unit - supposedly having
a significant range from transmitter to receiver. Was going to place the
transmitter by my windsock. Wrong! First Summer it became erratic. All
manner of flux residues and funky things growing inside the transmitter.
Don't know what flux was used, but they certainly used plenty of it. Was
difficult to clean, but doing so has resolved all the problems except for
range.
I have to go way further West to get to the board assembler. Two words come
to mind - cheap, chinchy. Pretty mediocre quality.
In my case, I did not get the value I expected to have paid for
Could the screw plating [under the head] have been poor? ... add flux
residues and humidity during shipment, and as Robert said - a wire beneath?
Steve Creswick
http://www.linkedin.com/in/stevencreswick
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Thursday, January 13, 2011 7:01 PM
To: [log in to unmask]
Subject: Re: [TN] a different Friday quiz
Inge,
I will take a wild guess, there is copper under the screw somewhere, right?
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Thursday, January 13, 2011 6:07 PM
To: [log in to unmask]
Subject: [TN] a different Friday quiz
I bought a digital temperature equipment, consisting of a inhouse table unit
and a outdoors unit. Cost = 25 USD. Cheap? Yes. But let's have a look on
inside after the problem, which started just a few weeks. You can read the
inside temperature, clock works, date works, and you can use the alarm and
shift between the four channels, but the receiver does not take in the
signals from the little sender on the wall any more. I dismantled the box
and marvelled when I saw the shit I payed for. It's a wonder that there are
any functions working at all! Now, what caused the dead receiver was a flow
of iron from one screw (upper left corner ) . There is a bridge of
corrosion products (brown and green) from the screw to the thermistor (RT)
continuing to the rest of the circuitry. When I washed the card and dried
it, the reciever worked again,
Now, folks, here comes a question for the sharp TNetters:
"How can the screw be so rusty and deliver iron ions when it's not connected
to anything? It's just torqued into the plastic body. The other screws are
identical, but have not been involved in anything. "
The box has been on the kitchen table and has not been exposed to humidity
or any else abnormal condition.
The two 1.5 V batteries are removed on the pics.
Hope the gregorian Steve will help me with the photos.
/Inge
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|