Hi, all:
在J-STD-001 中定义Non-RoHS 焊锡中含锡量的规格如下:
“对于用于预处理或组装的锡铅合金,其含锡量应当维持在所用合金标称值的±1%以内。”
我确认过英文版本,中英文的表达是一致的。
以常用的Sn63Pb37焊料为例,对于含锡量,我们目前有两种理解:
1。 63%Sn 的±1%变化,含锡量的规格下限为63%*(100%-1%)=62.37%; 规格上限为63%*(100%+1%)=63.63%; 所以规格为62.37%---63.63%
2。63%Sn ±1%变化。含锡量的规格下限为63%-1%=62%; 规格上限为63%+1%=64%; 所以规格为62%---64%
不知哪种理解忠实于标准,请各位不吝赐教!