Other than a lecture are there any good reasons?
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Monday, December 06, 2010 4:51 PM
To: [log in to unmask]
Subject: Re: [TN] HandSoldering Using NC Solders
Mike,
That's a big one. The answer is that you need to choose the best solder(s)
for your application(s). It is likely your two solders were selected by two
different people at two different times. When choosing materials, talking
to the manufacturers about the products, getting samples, and comparing them
head-to-head goes a LONG way. You must also consider reliability. The best
flux formulation is simply not the one that allows you to solder a rusty
nail to the hull of a ship. An important factor is how you plan to clean
your parts after soldering is all done, how well you can ensure you get all
the residues removed, and the potential impact of any residues remaining on
the assemblies. I suggest you start by reading through some tech articles
on cleaning. This forum, the industry magazines, Foresite, and ACI are some
good starting resources. Bottom line - you don't pick solder materials
solely on the basis of supplier or cost.
Good luck.
-----Original Message-----
From: Mike Laroe [mailto:[log in to unmask]]
Sent: Monday, December 06, 2010 4:06 PM
To: [log in to unmask]
Subject: [TN] HandSoldering Using NC Solders
Currently my company has been using two different Alloys for handsoldering
both Leaded and RoHs No-Clean Assy's. For the leaded requirement we are
using AIM and for Rohs we are using Kester. We currently stock 4 different
sizes of each (.015", .020", .025", .031").. My question and thought is to
phase out the AIM and strictly only use the Kester for both Leaded and Rohs
Assy's. All the Soldering is done with Metcals using the 700 & Pwr Tips.
Are there any reasons I shouldn't do this?
Thanks for your help in advance,
Mike Laroe
Mfg Engineer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|