TECHNET Archives

December 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Genny Gibbard <[log in to unmask]>
Date:
Sat, 11 Dec 2010 03:25:34 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, colin mcvean <[log in to unmask]>
Subject:
From:
colin mcvean <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (68 lines)
Hi Genny,
 
OSP older than 6 months is likely to show solderability issues, so the fact you have got 2 years is impressive.
 
Stripping the old OSP is simply a case of immersing the boards into 1 Sulphiric solution, and rinsing/drying well. It's unlikely to affect the Gold plating finish if it's been applied properly in the first place. New OSP coating can then be applied, also over the Gold plating. 
 
However...if the boards are too small, then the original supplier may have issues with being able to process them, especially if they have conveyorised equipment. Best to call the supplier and see if they can process.
 
Good luck
Colin

--- On Fri, 10/12/10, Genny Gibbard <[log in to unmask]> wrote:


From: Genny Gibbard <[log in to unmask]>
Subject: [TN] Old OSP
To: [log in to unmask]
Date: Friday, 10 December, 2010, 15:39


It seems to me that I have heard people say you can attempt to
rework/reclaim OSP finish boards that may have degraded?  Strip the
coating and the copper oxidation, and re-apply OSP?
We have a large stock of a PCBs with OSP finish that we were left with
when an OEM contract got severely reduced.  We have been whittling away
at the stock for the reduced orders, but now it is over 2 years old, and
we are starting to see problems with solderability.  
Would you go back to the original manufacturer for the rework process,
or would you go to some specialty house for this?
A wrinkle, possibly is that there are areas of selective gold plating as
well on the board.

Genny 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



      

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2