"UV has little known effects on Acrylics after more than 30 years exposure to full sunlight. Check acrylic "blinds" on factory doors."
I could be wrong but I thought acrylic yellowed in sunlight, which of course contains UV. Formulation could make a big difference of course.
If I've learned one thing about plastics it's always measure the properties of the grade you're using and don't trust a sales brochure or Matweb. You get huge differences between plastics that you'd expect to be much the same.
On 11/11/2010 14:56, Graham Naisbitt wrote:
> AT LAST, the chance is mine....
>
> It depends! (Hoisted by your own petard.)
>
> No papers to my knowledge, but you might check with Phil Kinner at HumiSeal, I recall we were involved in some "radiation effects" research, not UV specific but it might shed some light on the subject? (There's a "Deweyism" for you as well!)
>
> UV has little known effects on Acrylics after more than 30 years exposure to full sunlight. Check acrylic "blinds" on factory doors.
>
> As to the other coating types, you might need to ask at your DOD. Here in the UK our CDE at Porton Down ran some extensive investigations concurrently with the US DOD to determine NBC warfare resistance. Don't know if they'll give you any written answers though....
>
> Graham N
>
>
> On 11 Nov 2010, at 13:20, Douglas Pauls wrote:
>
>> Good morning all,
>>
>> Does anyone know of any papers on the effects of UV light on conformal
>> coating? Not talking the cosmic radiation hard space kind. I know it
>> would be wavelength and intensity specific. Got a question from one of
>> our engineers and I, of course, gave the very intelligent answer of "Beats
>> me". But I have this wonderful resourse called Technet...............
>>
>> Doug Pauls
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: http://listserv.ipc.org/archives
>> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> .
>
--
Eric Christison
Consumer& Micro group
Imaging Division
STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom
Tel: +44 (0)131 336 6165
Fax: + 44 (0)131 336 6001
The contents of the email are ST confidential.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|