TECHNET Archives

November 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 2 Nov 2010 15:17:51 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (80 lines)
I forget the details as this was going back to about 1970 but, in a 
former life, we did just this kind of thing to reduce barrel cracking. 
However, if I remember rightly, the electrolytic flash coating was only 
about 5 µm. I forget which order they came in but the flash coating and 
the 20 µm main plating were done in different baths, one being sulphate 
and the other pyrophosphate. The theory behind it is that the main 
plating had a better throwing power, while the flash coating had a 
better adhesion to the electroless copper, because of epitaxial growth.

Again, if my memory serves me correctly, we used this technology for 
only a short while, perhaps 12 months, after which it was replaced by a 
single bath which had sufficient quality in both aspects to no longer 
justify the extra step. Remember that this was in the relatively early 
days of through hole plating, and finding the right solution (no pun 
intended) was quite an adventure.

I see no justification for doing this today – copper plating has come a 
long way in 40 years!

Brian

On 02/11/2010 06:16, Uppina Nagaraj wrote:
> Hi All,
>
> We have a low build electroless Copper plating for Through Hole
> metalization, which's giving around 0.5 to 0.6microns of Copper.
>
> The subsequent processes are pattern image printing followed by
> pattern plating (electrolytic copper plating).
>
> One of our customer has a requirement to do flash Copper plating
> (electro plating) of around 8 to 10 microns, immediately after
> electroless Copper plating, prior to pattern image printing.
>
> I want some inputs on the above.....
>
> Is there a distinct advantage on PTH reliability by having
> 8-10microns of electroplated copper immediately after
> electroless Copper plating.
>
> Will having additional flash plating have better Thermal
> stress&  Thermal Shock performance.
>
> Thanks!
> U.Nagaraj
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2