TECHNET Archives

November 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Victor G Hernandez <[log in to unmask]>
Date:
Sat, 20 Nov 2010 21:17:54 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
John Goulet <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (110 lines)
Infrared Technology, Laconia NH. Ed Fortuna 603 759-2953. 

He goes to factory close-out auctions, upgrades and rebuilds equipment. Has lots of hard to find parts and circuit boards for equipment. 

He has a huge wharehouse. 



JMW   Brian Ebbinger  Web www.jmw-inc.com , phone 507 864-7477, Rushford MN. 


----- Original Message ----- 
From: "Victor Hernandez" <[log in to unmask]> 
To: [log in to unmask] 
Sent: Friday, October 29, 2010 3:07:14 PM 
Subject: Re: [TN] Used Equipment Brokers 

LabX 

-----Original Message----- 
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo 
Sent: Friday, October 29, 2010 11:05 AM 
To: [log in to unmask] 
Subject: Re: [TN] Used Equipment Brokers 

dovebid 

-----Original Message----- 
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jana Carraway 
Sent: Friday, October 29, 2010 11:50 AM 
To: [log in to unmask] 
Subject: [TN] Used Equipment Brokers 

Greetings List, 

Can you guys recommend a couple used equipment brokers? 

Thank you, 
Jana Carraway 
____________________________________ 
Jana Carraway 
MSEI - Advanced Technology Group 
6024 S.W. Jean Road 
Lake Oswego, Oregon  97035 
503.697.5291, ext 1180 
email: [log in to unmask] 

______________________________________________________________________ 
This email has been scanned by the MessageLabs Email Security System. 
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________ 

--------------------------------------------------- 
Technet Mail List provided as a service by IPC using LISTSERV 15.0 
To unsubscribe, send a message to [log in to unmask] with following text in 
the BODY (NOT the subject field): SIGNOFF Technet 
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) 
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest 
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 
----------------------------------------------------- 

--------------------------------------------------------------------- 
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. 

______________________________________________________________________ 
This email has been scanned by the MessageLabs Email Security System. 
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________ 

--------------------------------------------------- 
Technet Mail List provided as a service by IPC using LISTSERV 15.0 
To unsubscribe, send a message to [log in to unmask] with following text in 
the BODY (NOT the subject field): SIGNOFF Technet 
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) 
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest 
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 
----------------------------------------------------- 

______________________________________________________________________ 
This email has been scanned by the MessageLabs Email Security System. 
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________ 

--------------------------------------------------- 
Technet Mail List provided as a service by IPC using LISTSERV 15.0 
To unsubscribe, send a message to [log in to unmask] with following text in 
the BODY (NOT the subject field): SIGNOFF Technet 
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) 
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest 
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 
----------------------------------------------------- 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2