Louis,
Boy have I got a lot to say on this one. I will outline a few items here
but would be very happy to have a phone conversation about what has
worked for me, what hasn't and the interesting problems I have run into.
The big three are:
-reliability vs cost,
-Spray Pattern vs what you want to accomplish,
-conveyor options, is what your transport thick, thin or other,
I have developer for Photo Coverlay that I paid very little for from one
of the off brand suppliers. I did this because I thought I would only be
running it about four hours a week. Five years later it is a workhorse
running about 14 hours a day and most weeks 6 days. It does everything I
asked it for and very low operation cost and very high up-time.
Often fine line spray patterns are interfered with by conveyor parts. I
hate it when a spray bar is directly over a set of conveyor wheels. Look
carefully at where spray bars are placed so they spray directly on your
work.
Conveyors are more important than you think. Make sure you talk to
someone who has a unit you are considering that is 5 years. If he has
more than 4 conveyor issues a year reconsider that source.
Be very aware of your space requirement. If you want a good process you
probably need more rinsing than you think. Rinses take up space. You can
get counter-flow options in your quote to save water.
good luck,
Chuck Brummer l 3M Manufacturing Engineer
3m Electronic Solutions Division--Flexible Circuits
8357 Canoga Ave. l Canoga Park, CA 91304-2605
(818) 734-4930
[log in to unmask] l www.3m.com l www.3mFlex.com
From:
Louis Hart <[log in to unmask]>
To:
<[log in to unmask]>
Date:
11/19/2010 07:10 AM
Subject:
[TN] horizontal processing equipment
Sent by:
TechNet <[log in to unmask]>
TechNetters, may I have comments or advice on buying horizontal
processing equipment? We may be looking for something here. Reliability
is, of course, the primary consideration but any information is likely to
be helpful. It may be best to contact me off line, according to TechNet
policy.
Louis Hart
Compunetics
Monroeville, PA
USA
[log in to unmask]<mailto:[log in to unmask]>
412-858-1272
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|