Rudy,
I will have an answer for you tomorrow.
Bev
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak
Sent: Thursday, October 28, 2010 4:57 PM
To: [log in to unmask]
Subject: Re: [TN] Required solvent for IPC-TM-650, Method 2.3.4
What do you want, one, or two liters?
Rudy Sedlak
--- On Thu, 10/28/10, Bev Christian <[log in to unmask]> wrote:
From: Bev Christian <[log in to unmask]>
Subject: Re: [TN] Required solvent for IPC-TM-650, Method 2.3.4
To: [log in to unmask]
Date: Thursday, October 28, 2010, 1:55 PM
Rudy,
That would be fantastic! I will get you shipping info tomorrow.
Bev
RIM
From: R Sedlak [mailto:[log in to unmask]]
Sent: Thursday, October 28, 2010 04:33 PM
To: TechNet E-Mail Forum <[log in to unmask]>; Bev Christian
Subject: Re: [TN] Required solvent for IPC-TM-650, Method 2.3.4
Bev: Because I am one helluva nice guy, I will make you a quart (I meant
liter) of this stuff.
One of our regular products is almost this, and has a small amount of
another solvent.
I will make you a liter or the 90% Limonene qs. surfactant. product, and if
you pay for the freight, it is free. I'll even make you 2 liters, if you
want. Have you had a better offer this week?
PS. the term "qs" is abbreviated Latin, meaning "Quantum Sufficio", or
enough to make up to 100%.
(The stuff is flammable, so if you can put up with delay, we WAY ahead in
shipping charges if we ship UPS ground, where we package in one liter
bottles, and do not have to declare it hazardous. If we ship air, we must
declare and it ain't cheep.)
Rudy Sedlak
RD Chemical Company
--- On Thu, 10/28/10, Bev Christian <[log in to unmask]> wrote:
From: Bev Christian <[log in to unmask]>
Subject: [TN] Required solvent for IPC-TM-650, Method 2.3.4
To: [log in to unmask]
Date: Thursday, October 28, 2010, 12:11 PM
TechNetters,
The IPC test Method, "Chemical Resistance, Marking Paints and Inks" calls
for a "terpene defluxer consisting of a minimum of 90% d-limonene and 10%
surfactant". One supplier says their minimum order is 3 GALLONS (U.S., I
presume.). But whether they are U.S. or imperial gallons, I will be dead,
let alone retired before we would use up all this stuff. Any suggestions at
to what I can buy in a small jar or spray can that meets the IPC requirement
that I can buy?
Bev
RIM
PS: Perhaps I am being anal, but shouldn't that read "a minimum of 90%
d-limonene with the remainder being surfactant"? Using 90% limonene and 10%
makes the use of the word "minimum" superfluous.
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]<[log in to unmask]>
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to
[log in to unmask]<[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<[log in to unmask]>: SET Technet NOMAIL or
(MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at
[log in to unmask]<[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|