Dear Colleagues
Thanks a lo for the first answers.
- No, the BGAs have not been reworked
- Most failures occur in the field, some are found after production
- We didn't find any separations after only printing solderpaste and soldering.
- It's not only the corner balls, the defects are found statistically in the array
Günter
>-----Ursprüngliche Nachricht-----
>Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Joyce Koo
>Gesendet: Mittwoch, 27. Oktober 2010 13:26
>An: [log in to unmask]
>Betreff: Re: [TN] Cracks in BGA solderjoints
>
>Spalling of the IMC? Are those reworked?
>--------------------------
>Sent using BlackBerry
>
>
>----- Original Message -----
>From: Inge [mailto:[log in to unmask]]
>Sent: Wednesday, October 27, 2010 07:17 AM
>To: [log in to unmask] <[log in to unmask]>
>Subject: Re: [TN] Cracks in BGA solderjoints
>
>I think it's not cracks in the BGA, but snacks in the BGA. At least what
>I
>found once
>/Inge
>
>
>----- Original Message -----
>From: "Grossmann, Guenter" <[log in to unmask]>
>To: <[log in to unmask]>
>Sent: Wednesday, October 27, 2010 9:36 AM
>Subject: [TN] Cracks in BGA solderjoints
>
>
>Hi Technetters
>
>I have an effect in BGA solder joints that I have never seen before.
>In microsections and in FIB preparations I see cracks between the IMC
>and a
>slightly darker region towards the Ni which I assume to be a P enriched
>zone
>of the Ni. However, the cracks are somewhere in the width of the solder
>joint and they are quite short running out to a row of pores that look
>somehow like Kirkendall voids.
>Is there still a possibility to place one or two pictures? Kim's IPC
>site
>doesn't work.
>
>Best regards
>
>Günter
>
>
>
>______________________________________________________________________
>This email has been scanned by the MessageLabs Email Security System.
>For more information please contact helpdesk at x2960 or
>[log in to unmask]
>______________________________________________________________________
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask]
>or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>______________________________________________________________________
>This email has been scanned by the MessageLabs Email Security System.
>For more information please contact helpdesk at x2960 or
>[log in to unmask]
>______________________________________________________________________
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------------------------
>This transmission (including any attachments) may contain confidential
>information, privileged material (including material protected by the
>solicitor-client or other applicable privileges), or constitute non-
>public information. Any use of this information by anyone other than the
>intended recipient is prohibited. If you have received this transmission
>in error, please immediately reply to the sender and delete this
>information from your system. Use, dissemination, distribution, or
>reproduction of this transmission by unintended recipients is not
>authorized and may be unlawful.
>
>______________________________________________________________________
>This email has been scanned by the MessageLabs Email Security System.
>For more information please contact helpdesk at x2960 or
>[log in to unmask]
>______________________________________________________________________
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|