I agree with the Osmium answer.
Osmium had the highest melting point in the platinum group.
Osmium tetroxide is also used in electronmicroscopy as a staining agent.
mark
mark
Mark Woolley |PTRL Laboratory | Avaya | 1300 West 120th Ave |
Westminster, CO 80234 USA |
Voice (Lab): (303) 538-2166 | email: [log in to unmask] |
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Thursday, October 21, 2010 1:01 PM
To: [log in to unmask]
Subject: [TN] NTC Friday Element Quiz - the Question
Hi folks - here is the Friday Element Quiz Answer:
The Question:
This element is the "least used" within its metallic "group". It is very
brittle and forms a volatile, toxic oxide species. One of its oxide
species is used as a staining agent to detect fingerprints. It is added
as
an alloy addition to increase hardness for a product most of us never
use
- premium quality fountain pen tips. What element is this?
Bonus Points - This element has the highest XXXX property of all of the
metallic elements. Name that property.
The winner of the quiz will get to put Clumpy to work for a week.
So far Clumpy has:
Week 1 Lamar Young, SCS Coatings
- accomplished nothing (drank lots of coffee)
Week 2 Bev Christian, RIM
- conducted REACH material testing
Week 3 Drew Meyer, Benchmark Electronics Inc.
- Solderability testing and mowed the lawn
Week 4 Ian Fox, Goodrich
- had an epic journey of travel
Week 4 Gary Ferrari, Garrick Global
- ???? Gary owes us a description
Week 5 Fredrick Miller, Astrolab
- ???? Fredrick owes us a description
Week 6 David Nelson, Raytheon
- Was a tackling dummy for Dallas Cowboys
Week 7 Graham Collins, L3 Communications
- Cleaned gutters and painted window trim
Week 8 Bill Noel, ITT Geospatial Systems Division
- ???? Bill owes us a description
Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|