What about if you are testing an underfill?
Bev
-----Original Message-----
From: Joe Russeau [mailto:[log in to unmask]]
Sent: Thursday, October 14, 2010 4:01 PM
To: TechNet E-Mail Forum; Bev Christian
Subject: Re: [TN] Interpretation of SIR Requirements
Bev,
For the Telcordia document, the sample groups are defined in table 13-3 in
my copy and a description of the sample groups follows that table.
For the J-STD-004 B version, EVERY SIR value for processed samples must
maintain above 100 megohms. Keep in mind that the J-STD-004 B version is
now calling out the new SIR method 2.6.3.7, which is continuous monitoring
(every 20 minutes). The old 2.6.3.3 method had only five measurement sets
taken and only two counted towards passing the test (96 and 168 hours).
With the new method more measurements are taken and require more data
evaluation. That said, the IPC SIR TG has agreed that when method 2.6.3.7
is used a 24-hour grace period should be given before any data starts to
count due to the boards acclimating to the test conditions. The same
comments have also been made by flux TG about a 24-hour grace period. I
always give a 24-hour grace period when performing per J-STD-004, unless I
don't see any sort of recovery in the SIR results after 24-hours. If they
maintain below the pass limit after 24-hours, then I spend the time visually
inspecting for a root cause.
I hope this helps you.
Best Regards,
Joe Russeau
----- Original Message -----
From: "Bev Christian" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, October 14, 2010 2:29 PM
Subject: [TN] Interpretation of SIR Requirements
> TechNetters,
> In GR-78-CORE, Issue 1, 1997, SIR Test Procedure 13.1.3.2 R13-6 [808], it
> states (capitalization mine) "The average insulation resistance (megohms),
> for EACH SAMPLE GROUP, taken at 24 hours and again at 4 days, shall be
> greater than the minimum specified in table 13-4.
>
> In IPC J-STD-004B, 3.4.1.4.1 Reporting SIR Test Results, the first
> criteria for passing the SIR test is: "All SIR measurements on all test
> patterns shall exceed the 100 Mohm requirements."
>
> My questions are as follows:
> 1) In the Telecordia document, what constitutes a "sample group"? One comb
> pattern? All the comb patterns on one coupon? All the coupons being used
> to test one material?
> 2) For the IPC method does the criteria apply to the readings at the end
> of the test? First and last? At every measurement? The document seems
> vague to me.
>
> Bev
> RIM
>
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential
> information, privileged material (including material protected by the
> solicitor-client or other applicable privileges), or constitute non-public
> information. Any use of this information by anyone other than the intended
> recipient is prohibited. If you have received this transmission in error,
> please immediately reply to the sender and delete this information from
> your system. Use, dissemination, distribution, or reproduction of this
> transmission by unintended recipients is not authorized and may be
> unlawful.
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|