Hello Listers,
Has anyone had experience with MSA residues on electronic components or
MSA breakdown residues from a 90Sn/10Pb plating bath? Have any papers
been written addressing breakdown products or residues possible if poor
rinsing is involved? Any MSA type bath suppliers on the list who might be
willing to talk to me?
Thank you for any and all references,
Jana Carraway
____________________________________
Jana Carraway
MSEI - Advanced Technology Group
6024 S.W. Jean Road
Lake Oswego, Oregon 97035
503.697.5291, ext 1180
email: [log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------