TECHNET Archives

October 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 28 Oct 2010 12:42:10 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dennis Fritz <[log in to unmask]>
Subject:
From:
Dennis Fritz <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
<1715F6A348D944AD879F9B51F7CAD5ED@EngDan>
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (139 lines)
Sorry there is no simple answer - you will have to make some assumptions, or mark up your print to use specific imaging technology. 

First, trace shape depends on the etch resist used - photoresist or metallic electroplate.  If the fab process uses photoresist for the tent-and-etch process, the trace shape will be trapezoid, just as with inner layers.  

If the etch resist is metallic, the copper cross section depends on the thickness of the photoresist used, and unfortunately the resulting copper shape may not be consistent across the same board. Typically, the photoresist does not fully contain the plating and results in a cross section "mushroom".  The most complicated is when the pattern plated copper first mushrooms over the top of the resist, and then is covered by a metallic resist like tin electroplate.  A few shops may still use tin-lead electroplate, The most complicated would be nickel metallic etch resist that is stripped off - fortunately not common.  

The photoresist is stripped away before etching the starting copper foil on the surface.  Etchant attacks the sides of the traces, but with spray etching, to a lesser degree than etching "downward" on the starting foil.  Metallic etch resists cause a small amount of "galvanic attack" at the junction of the metal and the copper.  Nickel or nickel/gold junction with copper casuse a lot of galvanic attack, and much undercut. Tin or tin/lead has more galvanic attack than inert tenting photoresist, but much less than nickel.  It is never wise to fabricate so that etchant causes slivers of metal to crack off the edges of the circuit trace. 

Finally, the copper thickness on a board may vary with current density - thicker at board edges and isolated traces - where it may mushroom.  Where the traces are close together and near the center of the board, there will be the trapezoids you describe.  Starting with thin foil - half ounce or less - and using thick photoresist will make for more consistent copper cross sections. 

Denny Fritz






-----Original Message-----
From: Dan Skweres <[log in to unmask]>
To: TechNet <[log in to unmask]>
Sent: Thu, Oct 28, 2010 11:04 am
Subject: Re: [TN] profile (section) of outside layer trace


Mark,
hen we calculate impedance we typically have the foot of the trace wider 
han the top.The mushrooming of the trace actually depletes or breaks off 
hen tin stripping or resist stripping.
an S.
---- Original Message ----- 
rom: "Mark Larson" <[log in to unmask]>
o: <[log in to unmask]>
ent: Thursday, October 28, 2010 10:48 AM
ubject: Re: [TN] profile (section) of outside layer trace

ortobello? or ... I hope not morel
he reason I am asking is for impedance calculation, and I guess the 
ushroom shape is another reason to go stripline, better control 
prediction) of the finished line shape
-----Original Message-----
rom: Joyce Koo [mailto:[log in to unmask]]
ent: Thursday, October 28, 2010 9:14 AM
o: [log in to unmask]; Mark Larson
ubject: Re: [TN] profile (section) of outside layer trace
Mushroom.
-------------------------
ent using BlackBerry

---- Original Message -----
rom: Mark Larson [mailto:[log in to unmask]]
ent: Thursday, October 28, 2010 10:01 AM
o: [log in to unmask] <[log in to unmask]>
ubject: [TN] profile (section) of outside layer trace
during etching a trapezoid shape is created right? with long side of
rapezoid up (away from dielectric)? but after plating?
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
or additional information, or contact Keach Sasamori at [log in to unmask] or 
47-615-7100 ext.2815
----------------------------------------------------
---------------------------------------------------------------------
his transmission (including any attachments) may contain confidential 
nformation, privileged material (including material protected by the 
olicitor-client or other applicable privileges), or constitute non-public 
nformation. Any use of this information by anyone other than the intended 
ecipient is prohibited. If you have received this transmission in error, 
lease immediately reply to the sender and delete this information from your 
ystem. Use, dissemination, distribution, or reproduction of this 
ransmission by unintended recipients is not authorized and may be unlawful.
____________________________
his email has been scanned.
________________________________________________________
his email has been scanned. This e-mail (including any attachments) is 
onfidential and may be legally privileged. If you are not an intended 
ecipient or an authorized representative of an intended recipient, you are 
rohibited from using, copying or distributing the information in this 
-mail or its attachments. If you have received this e-mail in error, please 
otify the sender immediately by return e-mail and delete all copies of this 
essage and any attachments.
______________________________________________________________________
his email has been scanned by the MessageLabs Email Security System.
or more information please contact helpdesk at x2960 or [log in to unmask]
_____________________________________________________________________
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
or additional information, or contact Keach Sasamori at [log in to unmask] or 
47-615-7100 ext.2815
----------------------------------------------------

_____________________________________________________________________
his email has been scanned by the MessageLabs Email Security System.
or more information please contact helpdesk at x2960 or [log in to unmask] 
_____________________________________________________________________
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
dditional information, or contact Keach Sasamori at [log in to unmask] or 
47-615-7100 ext.2815
----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2