TECHNET Archives

October 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 27 Oct 2010 15:13:56 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Subject:
From:
Steve Gregory <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (243 lines)
Hi Bob,

Got everything posted. I shortened the file names somewhat so they wouldn't
wordwrap.

I had never seen Terry Munson's paper on fluid entrapment before, quite an
eye-opener!

http://stevezeva.homestead.com/Xilinx_xapp426.pdf

http://stevezeva.homestead.com/Vented_FCBGA_Fluid_Entrapment.pdf

http://stevezeva.homestead.com/Flip_chip_package_construction.pdf

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Landman
Sent: Wednesday, October 27, 2010 2:44 PM
To: [log in to unmask]
Subject: Re: [TN] Washing boards

And not all parts are sealed.  Take for example some flip chip FPGAs who's
lids are vented. 

I'm sending Steve Gregory documents illustrating some of the things that can
happen when washing boards with anthing more than DI water (and a
manufacturer's recommendation to not use "cleaning agents" - either no-clean
or water washable flux).  

Some on the tin whiskers telecon today were concerned that even DI water
washing can end up driving contaminants from the flux residue into the
vents.

Bob Landman
H&L Instruments, LLC


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Wednesday, October 27, 2010 2:09 PM
To: [log in to unmask]
Subject: Re: [TN] Washing boards

Perhaps, but I have found in the past that there is no such thing as a
totally hermetic sealed unit.  At least consistently.

Doug Pauls



Joyce Koo <[log in to unmask]>
10/27/2010 01:03 PM

To
'TechNet E-Mail Forum' <[log in to unmask]>, "[log in to unmask]" 
<[log in to unmask]>
cc

Subject
RE: [TN] Washing boards






Not part sealed, but system sealed... because he want everything washable...
possibly cheaper to seal the system... 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Wednesday, October 27, 2010 2:02 PM
To: [log in to unmask]
Subject: Re: [TN] Washing boards

Yannick,
There is almost no way to answer your general question accurately. 
Compatibility with most cleaning agents is not something you will find on
data sheets, since it will almost always depend on the combination of
cleaning agent and cleaning parameters. 

You can often ask the component vendor if they have any data on compatiblity
with a particular cleaning agent, or if you can get to the technical people,
ask whether the materials of construction are compatible 

with with the cleaning process proposed.

I would disagree with Joyce's comment that you are OK if the package is
hermetic.  This might keep the internal dies away from the cleaning agents,
but there are often exterior considerations, like part markings or 

attack on the component seals.

Doug Pauls



Yannick Brisson <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
10/27/2010 12:41 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to Yannick Brisson
<[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Washing boards






 Hi, 

                 I need to find for all (almost all) parts in our system 
if they
can go in the washer?  I look over a couples of part but I don't see any
info in the spec sheet, Do ou guys find something on that topics? Or do
you ask the manufacturer each time you have a new part ?

 

Thank You

Yannick

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 

for additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential 
information, privileged material (including material protected by the 
solicitor-client or other applicable privileges), or constitute non-public 
information. Any use of this information by anyone other than the intended 
recipient is prohibited. If you have received this transmission in error, 
please immediately reply to the sender and delete this information from 
your system. Use, dissemination, distribution, or reproduction of this 
transmission by unintended recipients is not authorized and may be 
unlawful.



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2