Thu, 21 Oct 2010 12:42:00 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (707 lines)
 Hi Bev,
You are right, I was thinking PCB only.
That king of quality certainly is possible, but at much lower plating rates.
Werner

 


 

 

-----Original Message-----
From: Bev Christian <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, Oct 21, 2010 12:31 pm
Subject: Re: [TN] Want to buy electrolytic copper foil


Werner,

You are thinking in only the PCB space.  I have in my hot little hands a 

cardboard tube from EM Science that was filled with “Copper ACS Foil, 

Electrolytic”.  And as you probably know ASC standards for the American Chemical 

Society and adding that to the label of your material is pretty serious 

business.  The assay beside the main title portion of the label says Assay Min 

99.9% and then it goes on to list the impurities, all at very low levels. So 

there does indeed appear to exist electrolytic copper in the purity range I 

asked about.

Bev

RIM

From: Werner Engelmaier [mailto:[log in to unmask]]

Sent: Wednesday, October 20, 2010 5:58 PM

To: [log in to unmask]; Bev Christian

Subject: Re: [TN] Want to buy electrolytic copper foil



Hi Bev,

Electrolytic copper foil of at least 99.9% purity is essentially a contradiction 

in terms. Commercial electrolytic Cu foil is plated at very high plating current 

densities—for reasons of economy, of course, which requires quite a witches brew 

of organic and other additives to be able to plate Cu with good physical 

properties and at a high rate. Some of these organics plate out on the grain 

boundaries, and that is the reason why Cu foil is sold by weight [oz/ft2] and 

with approximate thickness—the density is a variable.



Werner

Upcoming workshops:

September 21, European Electronics Assembly Reliability Summit, Tallinn, 

Estonia,

      “Solder Joint Reliability-Part 1: Fundamentals in Solder Joint 

Reliability”

September 21, European Electronics Assembly Reliability Summit, Tallinn, 

Estonia,

      “Solder Joint Reliability-Part 2: Failure Mode and Root Cause Analyses 

(Fatigue, Brittle Fracture, ENIG)”

November 2 & 9, SMTA Webtorial,

     “Fundamentals in Solder Joint Reliability”

December 7 & 14, SMTA Webtorial,

     “Acceleration Models, Accelerated Reliability Tests and Screening 

Procedures”









-----Original Message-----

From: Bev Christian <[log in to unmask]>

To: [log in to unmask]

Sent: Wed, Oct 20, 2010 2:26 pm

Subject: [TN] Want to buy electrolytic copper foil



TechNetters,















Where can I buy a roll of 0.002" thick electrolytic copper foil of at least















99.9% purity?















Bev















RIM





























---------------------------------------------------------------------















This transmission (including any attachments) may contain confidential















information, privileged material (including material protected by the















solicitor-client or other applicable privileges), or constitute non-public















information. Any use of this information by anyone other than the intended















recipient is prohibited. If you have received this transmission in error, please















immediately reply to the sender and delete this information from your system.















Use, dissemination, distribution, or reproduction of this transmission by















unintended recipients is not authorized and may be unlawful.





























______________________________________________________________________















This email has been scanned by the MessageLabs Email Security System.















For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>















______________________________________________________________________





























---------------------------------------------------















Technet Mail List provided as a service by IPC using LISTSERV 15.0















To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with 

following text in















the BODY (NOT the subject field): SIGNOFF Technet















To temporarily halt or (re-start) delivery of Technet send e-mail to















[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)















To receive ONE mailing per day of all the posts: send e-mail to















[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest















Search the archives of previous posts at: http://listserv.ipc.org/archives















Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for















additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> 

or















847-615-7100 ext.2815















-----------------------------------------------------















---------------------------------------------------------------------

This transmission (including any attachments) may contain confidential 

information, privileged material (including material protected by the 

solicitor-client or other applicable privileges), or constitute non-public 

information. Any use of this information by anyone other than the intended 

recipient is prohibited. If you have received this transmission in error, please 

immediately reply to the sender and delete this information from your system. 

Use, dissemination, distribution, or reproduction of this transmission by 

unintended recipients is not authorized and may be unlawful.



______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask] 

______________________________________________________________________


 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2