TECHNET Archives

October 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 20 Oct 2010 10:06:25 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (101 lines)
Hold on, Bob. Bad info.
No-clean flux residues from solder paste ARE inerted when they go through reflow. Most of the issues with no-clean flux are for benchtop liquid flux applications during rework or hand-soldering, which may not be fully inerted because the heat from a solder iron tip is not sufficient to do so, and because the liquid tends to run under places it was not intended to go. However, careful application of no-clean liquid fluxes using a felt-tip dispenser with a good operator are usually pretty safe.

No-clean solder pastes are used daily on circuit boards by the million, with few or no issues. While not favored for military or high-rel use, they work well in many other applications.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Landman
Sent: Wednesday, October 20, 2010 9:51 AM
To: [log in to unmask]
Subject: Re: [TN] Cleanable Long Stencil Time Flux Question

Bob K,

I'm sure this will ignite a debate but personally, I wouldn't allow any of our boards to be assembled with "no-clean" solder paste.  Perhaps Terry Munson can share with you some photos of why that's a bad idea.  Not all the flux is inerted by the reflow process, so I'm advised. 

Check out his website at http://residues.com/

This paper should give you some ideas
http://residues.com/pdfs/Circuits%20Assembly%20Articles/2004/low%20res/2004.03-The%20Key%20to%20Success%20-%20Circuits%20Assembly.pdf

Also this one
http://residues.com/pdfs/Circuits%20Assembly%20Articles/2003/low%20res/2003.03-Component%20Cleanliness%20in%20a%20No-Clean%20World%20-%20Circuits%20Assembly.pdf

I've visited Terry's facility in Kokomo, IN.  He's got an incredible array of diagnostic instrumentation, some of which he has designed and manufactured himself (like the C3).

Bob Landman
H&L Instruments, LLC


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Wednesday, October 20, 2010 10:10 AM
To: [log in to unmask]
Subject: [TN] Cleanable Long Stencil Time Flux Question

Can anyone make a paste/flux suggestion?

 

 In a past life I once used a No Clean Alpha Metal 6106 paste which had an incredibly long stencil life, I think it was 8 hours.

 

 This stuff never really "Dried Out" and a pasted board could sit for two days and a "Missing Part" could thus be ordered and reflow soldered.

 

 Trouble was NOTHING would remove this no clean flux and trying to wash messy THT or Rework flux could make a real mess.

 

 Can anyone suggest a cleanable paste/flux that has a long stencil life and does not dry out to a hard crust?

 

Thanks,

Bob K.



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2