Hi All,
I sent a link to the wrong, but in many ways, a better paper. The paper
that is in the link is "Thermal Cycle Testing" by Mike Freda and me.
This paper addresses the effects of lead free also and is a more
comprehensive paper.
The end of the paper addresses some of the effects of lead-free testing.
Table one is a reasonable overview of the effect of lead-free assembly
on PTH reliability.
http://www.circuitmart.com/pdf/thermal_cycle_testing.pdf
Sincerely,
Paul Reid
Program Coordinator
PWB Interconnect Solutions Inc.
235 Stafford Rd., West, Unit 103
Nepean, Ontario
Canada, K2H 9C1
613 596 4244 ext. 229
Skype paul_reid_pwb
[log in to unmask] <mailto:[log in to unmask]>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: September 27, 2010 1:52 PM
To: [log in to unmask]
Subject: Re: [TN] Leadfree Plated Thru Hole Thermal Cycle Reliability
Paper Hunt
Hi Paul,
This link does not work [for me]---can you send me the paper?
Werner
-----Original Message-----
From: Paul Reid <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, Sep 27, 2010 1:46 pm
Subject: Re: [TN] Leadfree Plated Thru Hole Thermal Cycle Reliability
Paper Hunt
Hi Dave,
I wrote a paper back in 2007 "PWB Reliability - the next step". It was
originally published by the Emerald Group. It looks like the Emerald
Group wants to charge to read the paper but here is a link where the
paper is available at no charge.
http://www.circuitmart.com/pdf/thermal_cycle_testing.pdf
This may be of interest. It shows the thermal cycles to failure in PTHs
are reduced by about 50% due to lead/free assembly on well fabricated
PWBs.
Sincerely,
Paul Reid
Program Coordinator
PWB Interconnect Solutions Inc.
235 Stafford Rd., West, Unit 103
Nepean, Ontario
Canada, K2H 9C1
613 596 4244 ext. 229
Skype paul_reid_pwb
[log in to unmask] <mailto:[log in to unmask]>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: September 23, 2010 12:31 PM
To: [log in to unmask]
Subject: [TN] Leadfree Plated Thru Hole Thermal Cycle Reliability Paper
Hunt
Hi folks! I am on a fishing exposition: I am looking for plated thru
hole
thermal cycle reliability reports/papers. I have a ton (literally) of
surface mount technology investigations but we have just finished up a
leadfree wave solder alloy thermal cycle solder joint integrity
investigation and I am in search of published data sets so I can do a
results comparison. I do have the papers by C. Hamilton/Celestica which
are very good but I am in quest of additional report data sets. If you
know of any published reports, please drop me an email.
Thanks in advance.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|