Totally agree Bob. We only hand-assemble through-hole. Don't do our own prototypes.
For limited SMT repair/rework we use water-washable and go through the same process.
Never have tried to remove a BGA myself - I let the CM do that. Fortunately (knock on wood)
we have had very few failures in SMT assemblies so haven't had to do much rework/repair.
The only part we've had to remove/replace is the Analog Devices AD208 (RS-232 interface) as even with transorb
zener protection, occasionally a customer smokes one of them. We're in the electric utility industry
and sometimes lightning can take out a unit and it's always the interface that fails. Happens when the customer
doesn't do the grounding correctly.
Bob Landman
H&L Instruments, LLC
On Sep 8, 2010, at 3:32 PM, Robert Kondner wrote:
> Bob,
>
> Try a "Water Pick" from a drug store, I got one at Walmart. I use it after
> rework of a small part, it really blasts water under parts. I fill the
> container with hot water and blast under small SMT parts. For complete board
> wash I use a spray assembly like found on a kitchen sink.
>
> This is ok for protos but a real washing system would be suggested for
> production. It takes a long, good, hot spray to get under BGAs. For QFNs
> forget it, you can not clean under those parts. Cleaning solutions are a big
> help.
>
> Also:
>
> I did not see any comments on my analyses of using tap water. Even with
> 500mg / L dissolved solids tap water it takes a good number of small drops
> to push towards the 10ug/insq limit. A 1mm drop (1/2 sphere) per 1 inch sq
> is only .25 ug/insq. It would take 40 drops per inch square and THAT is a
> lot of tap water. A quick blow off with an air gun leaves much less.
>
> Bob Kondner
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Landman
> Sent: Wednesday, September 08, 2010 5:18 PM
> To: [log in to unmask]
> Subject: Re: [TN] Hand Soldering
>
> We switched to water-soluble Kester brand and are very satisfied with it.
> Hot water and a good brush (we use a dish washing brush).
>
> Bob Landman
> H&L Instruments. LLC
>
> On Sep 6, 2010, at 6:30 AM, Kenneth Wood wrote:
>
>> Hi all.
>> What is the best setup for hand soldering as far as solder / cleaner?
>> Rosin core? Water soluble? No-Clean?
>> What cleaner too?
>>
>> I've been using rosin core with various cleaners but I have a hard time
> with
>> the white residue the cleaners leave.
>>
>> Thanks
>> Ken
>>
>>
>>
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: http://listserv.ipc.org/archives
>> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|