TECHNET Archives

September 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Landman <[log in to unmask]>
Date:
Thu, 9 Sep 2010 07:12:44 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Douglas Pauls <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (276 lines)
Good morning Bob,
Yes, you do have to be concerned with the plastics that you use and you 
have to match it to the cleaning solution used.  I don't think we have 
seen any incompatibility issues for either the Flux Off or the Kyzen 
cleaners, but then we are building Class 3 avionics and military products 
and may be dealing with a slightly higher grade of component.  On the 
other hand, the cost accounting weasels keep pushing us to cheaper and 
cheaper parts, so we have to keep an eye on it.

Doug Pauls



Bob Landman <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
09/08/2010 04:30 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Bob Landman <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Hand Soldering






Doug,

My one concern with any chemical cleaners such as Chemtronics is what they 
can do to
plastics.  The HP 8 segment alphanumeric displays we use were cracked by 
using anything
but hot water to remove flux.  We sent a cracked display to HP (now Avago) 
and they
told us this was the problem and pointed to the datasheet caution:

Soldering and Post Solder Cleaning Instructions for the 
HDSP-210X/-211X/-250X

The HDSP-210X/-211X/-250X may be hand soldered or wave soldered with SN63 
solder. When hand soldering, it is recommended that an electronically 
temperature controlled and securely grounded soldering iron be used. For 
best results, the iron tip temperature should be set at 315°C (600°F). For 
wave soldering, a rosin-based RMA flux can be used. The solder wave 
temperature should be set at 245°C ± 5°C (473°F ± 9°F), and the dwell in 
the wave should be set between 11 /2 to 3 seconds for optimum soldering. 
The preheat temperature should not exceed 105°C (221°F) as measured on the 
solder side of the PC board.

For additional information on soldering and post solder cleaning, see 
Application Note 1027, Soldering LED Components.

Bob Landman
H&L Instruments, LLC



On Sep 7, 2010, at 7:13 AM, Douglas Pauls wrote:

> Ohhhh, I beg to differ.  Water soluble fluxes are more active and will 
> probably do OK for soldering, but they also represent a danger if you do 

> not totally remove them or if some of it flows into places and does not 
> get rinsed out.  What really makes me nervous about your approach is 
your 
> choice of equipment and cleaners. Tap water sucks as a cleaner and hot 
tap 
> water only slightly better.  You might be able to remove the visible 
> residues, but will still have invisible residues that will cause 
problems. 
> In some cases, you are putting on more contaminants with the tap water 
> than you are removing.
> 
> We use low residue fluxes here on class three product and have a number 
of 
> cases where the the residues are left in place.  It is simply a matter 
of 
> finding a flux and cleaning combination that works well together, and 
> limiting the amount of additional flux you add.  A skilled operator can 
do 
> soldering with no more flux than is in the core of the wire. You may 
need 
> a slightly larger core.
> 
> Ken, I would suggest this short list to you.  Use either Kester 245 low 
> residue flux (P3 core) or Alpha Telecore Plus (also P3 core).  Both are 
> standards here and work well for soldering.  For topical cleaning 
> solutions, try Kyzen's Cybersolv 141b or Chemtronics Flux-Off Heavy 
Duty. 
> Both these cleaning agents work well with the fluxes I named. 
> 
> Doug Pauls
> Rockwell Collins
> 
> 
> 
> Robert Kondner <[log in to unmask]> 
> Sent by: TechNet <[log in to unmask]>
> 09/06/2010 01:27 PM
> Please respond to
> [log in to unmask]
> 
> 
> To
> [log in to unmask]
> cc
> 
> Subject
> Re: [TN] Hand Soldering
> 
> 
> 
> 
> 
> 
> Ken,
> 
> In my mind there is absolutely no question, hand assemble using Water
> Soluble flux. A good spray under hot water cleans well. 
> 
> During final assembly or rework I might use a no clean at spots. The 
only
> problem is the no clean is VERY DIFFICULT to remove so don't try. It
> detracts from board appearance.
> 
> It the spot being reworked is a sensitive analog circuit they rework 
> using
> Water Soluble. For anything close to fine pitch SMT you should be 
applying
> liberal quantities of Water Soluble flux, only way to rework.
> 
> You can get a little "Water Pick" real cheap. Load it with hot water and
> you can you can really get down into the nooks and crannies. 
> 
> Bob Kondner
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Kenneth Wood
> Sent: Monday, September 06, 2010 8:30 AM
> To: [log in to unmask]
> Subject: [TN] Hand Soldering
> 
> Hi all.
> What is the best setup for hand soldering as far as solder / cleaner?
> Rosin core? Water soluble? No-Clean?
> What cleaner too?
> 
> I've been using rosin core with various cleaners but I have a hard time 
> with
> the white residue the cleaners leave.
> 
> Thanks
> Ken
> 
> 
> 
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
[log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text 
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
http://listserv.ipc.org/archives
> Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] 
or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
[log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text 
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
http://listserv.ipc.org/archives
> Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] 
or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
[log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text 
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
http://listserv.ipc.org/archives
> Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
ext.2815
> -----------------------------------------------------
> 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2