We need paste to print and reflow.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Goulet
Sent: Thursday, August 12, 2010 11:13 AM
To: [log in to unmask]
Subject: Re: [TN] SAC 95.5-3.5-1
If your not a manufacturing shop then you probably aren't looking for bar solder for a solder pot of any kind.
If your request was for the solder spec., as written in your E-mail and no mention or flux, then they are quoting bar solder which comes in 2+lb bars and about 20-30lbs boxes.
You can definitely buy a roll of core solder ffor a handsolder operation. Here are some of the many suppliers: from Contact East, Marshal, The WaveRoom Plus, EIS, etc.
You just have to specify the flux type for the core, OA (need to wash), No Clean (leaves a residue) and then the agressiveness of the flux depending on your application. Then you can hand solder your school project boards.
----- Original Message -----
From: al shirazi <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, 12 Aug 2010 14:42:29 -0000 (UTC)
Subject: Re: [TN] SAC 95.5-3.5-1
Have you tried All-spec?
Al
________________________________
From: Syed Ahmad
To: [log in to unmask]
Sent: Thu, August 12, 2010 10:26:17 AM
Subject: [TN] SAC 95.5-3.5-1
We are not a manufacturing house and are looking for small amount of SAC
95.5-3.5-1 for evaluation. We are receiving $1,000+ quotes for a minimum
order of a kilogram while we do not need that much. Usually we can get free
samples for evaluation but this one is proving to be a tough one. Any
suggestions?
Thanks.
Syed Sajid Ahmad, Center for Nanoscale Science and Engineering (CNSE)
North Dakota State University (NDSU)
http://www.ndsu.edu/cnse/
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|