Of course I looked it up. I don't think we need a word for that.
But, Clumpy is a better word.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Naisbitt
Sent: Tuesday, August 10, 2010 5:59 AM
To: [log in to unmask]
Subject: Re: [TN] blumpy (codeposited organics)
Ahem. Please do NOT use the term "Blumpy" - it has a meaning in the slang
dictionary that you REALLY don't want to know!
Having taken a look at Chris's photo, I think the correct term might be
"Clumpy - having or showing a tendency to form clumps"
Clump = as a noun: a compacted mass or lump of.... as a verb: to form into a
mass or clump
Graham N
On 6 Aug 2010, at 23:23, Chris Mahanna wrote:
> I'm not giving up the secret, but it is the same way that you use a
metallograph to tell which way the train was moving.
>
> I have loose parts and they are definitely not Ni/Pd/Au. Nor is there any
indication of insufficient heat on the surrounding parts. Actually my first
response to the customer was incomplete coalescence due to lack of flux
activity. But he didn't like that answer, because he knew it was only
related to that batch of parts. So, I went back and looked up Rich
Kraszewski's recipe for smoking out organics.
> At the moment, I'd say there is a good chance they are counterfeit parts,
but they might just be really old and contaminated...?
> Anyhow, since no one objected, I'm going to use the term blumpy in the
report.
>
> Have a great weekend everyone.
>
> Chris
>
> From: [log in to unmask] [mailto:[log in to unmask]]
> Sent: Friday, August 06, 2010 4:27 PM
> To: TechNet E-Mail Forum; Chris Mahanna
> Subject: Re: [TN] blumpy (codeposited organics)
>
>
> I'm just curious how Chris got a freight train under a
microscope...............
>
> Doug Pauls
>
> Chris Mahanna <[log in to unmask]>
> Sent by: TechNet <[log in to unmask]>
>
> 08/06/2010 12:39 PM
> Please respond to
> TechNet E-Mail Forum <[log in to unmask]>; Please respond to
> Chris Mahanna <[log in to unmask]>
>
>
> To
>
> [log in to unmask]
>
> cc
>
> Subject
>
> [TN] blumpy (codeposited organics)
>
>
>
>
>
>
>
> So a customer has the blumpies. The hand (dry) solder melt-front smokes
like a freight train under the microscope.
>
>
>
> My questions are:
>
>
>
> Have we really coined "blumpy"? and
> If it wets and forms proper fillets, is it conformant?
>
> Thanks!
> Chris
>
> Click here<https://robisan.sharefile.com/d-s8f0852004d94e529> to download
attachments.
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|