Hi,
Other than he color is there a problem with the boards?
Bob Kondner
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tan Geok Ang
Sent: Monday, August 09, 2010 9:47 PM
To: [log in to unmask]
Subject: Re: [TN] PCB Discoloration
Believed that these boards might have/ were "jammed thus heated" within
the wave soldering process which resulted in this issue?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Krishnan
(Radhakrishnan) Chezhian
Sent: Tuesday, 10 August 2010 6:54 AM
To: [log in to unmask]
Subject: Re: [TN] PCB Discoloration
Hi All,
This is a double sided board, we did not see this defect when the boards
were shipped. This is a pretty straight forward process for double sided
boards with red soldermask. The only heat cycle it sees is during the
soldermask pre-cure and final cure. So based onour records and data we
did
not see any abnormality during the curing process. Also the only other
area
we suspected was at final visual inspection where an inspector found
exposed
copper and touched-up the copper surface with mask and wanted to bake
it. So
we baked a board at 250F for 60 hours, simulating extreme conditions and
did
not see any discoloration, at least to this extent.
We are not sure what processes the boards go through at the assembler in
Jabil Shanghai, we are getting back some baords for FA. So we are open
to
resolve this issue ad if anyone has any suggestions pls feel free to
comment.....
Thanks,
Krishnan
On Tue, Aug 10, 2010 at 1:12 AM, Genny Gibbard
<[log in to unmask]>wrote:
> I am late into this discussion, since I have been on holidays, but did
> anyone consider the possibility that the layers were stacked together
in
> the wrong order internally? I have seen colour changes like that on
one
> batch that was made wrong. If the internal copper plane layer is
closer
> to one surface than it normally should be, it would appear darker on
one
> side and lighter on the other than normal, which is what I see with
the
> ring.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Skweres
> Sent: July 30, 2010 10:59 AM
> To: [log in to unmask]
> Subject: Re: [TN] PCB Discoloration
>
> Looks almost like one is FR-4 and the other is Polyimide. There was
> mention that they are from different lots. Call the supplier and see.
> Perhaps they (the board supplier) messed up and pulled one sheet of
> Polyimide and figured that it would be okay to send based on the fact
it
> met or exceeded requirements per print.
> Dan S.
> ----- Original Message -----
> From: "Steve Gregory" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Thursday, July 29, 2010 9:34 PM
> Subject: Re: [TN] PCB Discoloration
>
>
> > Hi Linda!
> >
> > While discoloration in itself is not a defect, I would be a little
> > worried about these seven boards. Especially since the rest of the
lot
>
> > are not discolored like this:
> >
> >
> > http://stevezeva.homestead.com/PCB_Discoloration1.jpg
> >
> >
> >
> > I don't see any delamination in the photos, but it sure looks like
the
>
> > boards got pretty toasty. I wonder if it was because the boards were
> > sitting over a preheater or hot plate too long. From the looks of
the
> > components on the board, most of it was probably hand soldered
(those
> > PTH caps converted to SMT couldn't have taken reflow), and I imagine
> > that the solid plane on on the backside of the board was a real
> heatsink.
> > Preheating the board would have helped with soldering the PEM nuts
for
>
> > sure, but maybe the preheater was set too high. I know a Hakko IR
> > preheater can smoke a board if you're not careful (not that I've
ever
> > done that, but I know a friend of a friend who did. Hehehehe).
> >
> >
> >
> > Anyways, those seven boards saw more heat than the rest of them did
> > based on the appearance in the photos. I don't think I'd buy off on
> them...
> >
> >
> >
> > Steve
> >
> >
> >
> >
> >
> >
> >
> > From: Linda Langley [mailto:[log in to unmask]]
> > Sent: Thursday, July 29, 2010 1:42 PM
> > To: Steve Gregory
> > Subject: FW: PCB Discoloration
> >
> >
> >
> > Hi Steve,
> >
> >
> >
> > Here I go again asking for help from my experts! Can you please post
> > these pictures? So I don't have to bother the whole forum, would you
> > know the name of the board guru that could answer my questions?
> >
> >
> >
> > I am not sure if the discoloration is a defect, is this a form of
> > delaminating? Why would only seven boards turn this color? They are
> > all from the same lot.
> >
> >
> >
> > Any information will be greatly appreciated.
> >
> >
> >
> >
> > Linda Langley CIT
> >
> > Training Specialist
> >
> > Jabil Circuit
> >
> > 248-292-6176
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or
[log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional
information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
CONFIDENTIALITY
This e-mail message and any attachments thereto, is intended
only for use by the addressee(s) named herein and may contain
legally privileged and/or confidential information. If you
are not the intended recipient of this e-mail message, you
are hereby notified that any dissemination, distribution or
copying of this e-mail message, and any attachments thereto,
is strictly prohibited. If you have received this e-mail
message in error, please immediately notify the sender and
permanently delete the original and any copies of this email
and any prints thereof.
ABSENT AN EXPRESS STATEMENT TO THE CONTRARY HEREINABOVE, THIS
E-MAIL IS NOT INTENDED AS A SUBSTITUTE FOR A WRITING.
Notwithstanding the Uniform Electronic Transactions Act or
the applicability of any other law of similar substance and
effect, absent an express statement to the contrary
hereinabove, this e-mail message its contents, and any
attachments hereto are not intended to represent an offer or
acceptance to enter into a contract and are not otherwise
intended to bind the sender, Sanmina-SCI Corporation (or any
of its subsidiaries), or any other person or entity.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|