A problem that used to occur when printed circuit boards were Tin/Lead plated happened when the board was left too long in a soak tank of acid immediately prior to Tin/Lead plating.
In that tank, the Copper substrate would react with dissolved Copper to form BAD tarnish. The board would still plate, but the plating would not be adherent.
(Problem was made worse, if acid tank was not changed out regularly, and dissolved Copper content was allowed to build.)
Is it possible you are getting this phenomenon? If a drop of fairly conc. Hydrochloric Acid dissolves black, it points to this being the problem.
Rudy Sedlak
RD Chemical Company
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|