Thanks, this is helpful. I was going to ask manufacturing to obtain the
actual temperature of the lead during the reflow process and then
measure it during hand soldering. I wanted to know if the temperature
of hand soldering was slightly higher allowing the wetting action to
improve. Jon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, August 24, 2010 4:13 PM
To: [log in to unmask]
Subject: Re: [TN] SOLDERABLIITY ON NICKEL PLATIUM GOLD LEAD FINISH SMT
PARTS
Hi Jon! There are a couple things to remember when dealing with NiPdAu
surface finishes: 1) Pd diffuses very slowly into a tin/lead solder
alloy.
You may need to add a few seconds to your soldering process cycle time;
2)
Adding an additional 5-10C of temperature will assist in the Pd
diffusion
into the tin/lead solder alloy. You may need to increase your soldering
temperature depending on which soldering process you are using; 3) Some
flux material are not compatible with Pd materials. You may want to try
a
different flux to see if you get an improved reaction; 4) Run a
solderability test per IPC JSTD 002 to make sure you have an acceptable
NiPdAu surface finish. When Texas Instruments first introduced the
NiPdAu
surface finish, we had to make slight time/temperature/flux adjustments
on
our typical soldering processes to obtain our expected soldering
results.
Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Roberts, Jon (SA-1)" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
08/24/2010 12:41 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Roberts, Jon (SA-1)" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] SOLDERABLIITY ON NICKEL PLATIUM GOLD LEAD FINISH SMT PARTS
Have any of you experience difficulty in producing an acceptable solder
joint with Nickel platinum gold SMT lead finishes? We can rework at
least twice to achieve an acceptable condition. Lead free part but we
use a solder with lead. Any help is appreciated. Jon
This communication is intended only for use by the addressee(s) named
herein and may contain business confidential and/or legally privileged
information. If you are not the intended recipient of this e-mail, you
are
hereby notified that any dissemination, distribution, disclosure or
copying of this e-mail and its contents is strictly prohibited. If you
have received this e-mail in error, kindly notify the sender by replying
to this message. In addition, please permanently delete the message and
any attachments without copying or disclosing the contents. Thank you
for
your cooperation.
THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR
TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE
EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE
APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR
DEPARTMENT OF COMMERCE.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|