The spec does not discriminate between electroless and electrolytic
therefore it is Cu plating and counts.
Jim
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Jose A
Rios
Sent: Wednesday, August 25, 2010 7:40 AM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] wrap and electroless
you cant see enough electroless in a microsection to measure it, even at
500 or 1000x unless you're really 'globbing it on'.
if you're counting on eless to meet the wrap requirement, thats a
loosing
proposition. at least for 'medium-build' eless chemistry setups.
in the event a 'high-build' eless application is employed, and the
deposit
is measurable, i dont see why you cant count it toward meeting the wrap
requirement....
Joey Rios
PWB & Process Quality Eng'r
Endicott Interconnect Technologies
1093 Clark St.
Endicott, NY 13760
Office: 607-755-5896
Chris Mahanna <[log in to unmask]>
Sent by: IPC-600-6012 <[log in to unmask]>
08/24/2010 08:52 PM
Please respond to
"(Combined Forum of D-33a and 7-31a Subcommittees)"
<[log in to unmask]>
To
[log in to unmask]
cc
Subject
[IPC-600-6012] wrap and electroless
another opinion poll, of sorts:
With even the most discriminating customers allowing 0.0002" wrap, and
huge aspect ratios leading to thicker electroless, the assumption that
wrapped electroless counts as wrap becomes more and more important. I
assume that everyone is counting it?
Thanks,
Chris
Chris Mahanna
President, Technical Manager
Robisan Laboratory Inc.
6502 E. 21st Street
Indianapolis, Indiana 46219
317-353-6249
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
NOTICE: This email message is for the sole use of the intended recipient(s) and may contain confidential and privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply email and destroy all copies of the original message.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|