TECHNET Archives

August 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Amol Kane <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 6 Aug 2010 10:09:56 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Subject:
From:
Steve Gregory <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<C23267C3AF7B4842B685FC757EE8A7B8491FEEDBD9@catvesexch01>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (44 lines)
Hi Amol!

I have your pictures posted:

http://stevezeva.homestead.com/IMG_8358.JPG

http://stevezeva.homestead.com/IMG_8359.JPG

http://stevezeva.homestead.com/IMG_8360.JPG

Steve

-----Original Message-----
From: Amol Kane [mailto:[log in to unmask]] 
Sent: Friday, August 06, 2010 9:35 AM
To: Steve Gregory; TechNet E-Mail Forum
Subject: Discoloration under the soldermask

Steve, would you be so kind to put them up on your site?....the
discoloration is underneath the soldermask. do any of you guys/gals know
what may cause this to happen?. this is across multiple date codes. I am
looking for a possible root cause so that I can decide whether or not to
reject these boards and issue a corrective action to the vendor.

Thanks!

Amol


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2