TECHNET Archives

August 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Mon, 23 Aug 2010 11:25:29 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Karen Tellefsen <[log in to unmask]>
Subject:
From:
Karen Tellefsen <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (48 lines)
Why would anyone want to underfill twice?  Was the initial underfill 
insufficient?  If so, isn't a second underfill a band-aid rather than a 
permanent solution to the problem?

What new problems would the second underfill cause?

Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069




From:   Bev Christian <[log in to unmask]>
To:     [log in to unmask]
Date:   08/23/2010 11:19 AM
Subject:        [TN] Double underfill
Sent by:        TechNet <[log in to unmask]>



Technetters,
I would like your opinions on a theoretical underfill situation.  What 
would be your comments be if a process group told you that they had 
underfilled a component and it was cured and they wanted to add more 
underfill to the component?
Bev
RIM

----



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2