TECHNET Archives

August 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ofer Cohen-QM <[log in to unmask]>
Date:
Wed, 4 Aug 2010 10:20:36 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Douglas Pauls <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (94 lines)
Ofer,
As Joyce said, they are costly for a reason.  But I think you will find 
that 1B31 and 1B73, as solvent based acrylics will be the more economical 
choices for hostile environments.  There are other urethanes or silicones 
that you might consider, but those are not as reworkable as the acrylics. 
Here are some of the "it depends" factors:

How important is rework and repair, or is this a throw away item?  If 
rework is not an issue, urethanes and silicones become more attractive.
Is this class 3 hardware and what are the consequences of failure?
When you say dust, moisture, and pollution, how dusty, how moist, and how 
polluted?  Chemical resistance becomes very important here.
What is the design life of the assembly?
How good is the enclosure around the assemblies you are coating?

I have design engineers ask me all the time if they can eliminate 
conformal coating, generally to take cost out of the unit.  I tell them, 
sure, as long as they are making a hermetic enclosure. They don't like 
that response.  For a hostile environment, you have to protect the 
electronics either with the enclosure or at the assembly level with 
coating.  Period.

Doug Pauls
Rockwell Collins




Ofer Cohen-QM <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
08/04/2010 09:59 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ofer Cohen-QM <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Conformal coating






Hello, technetters,
We are coating commercial products that are exposed to urban atmosphere of 
dust, moist and pollution with Humiseal 1B31 and 1B73. These are expensive 
materials. Are there any other coating materials that can be applied for 
this environment?

Thank you
Ofer Cohen


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2