I need some clarification on the requirement for Plating/Coating
Thickness. The 3/A page requires additional copper thickness above
class 3 to be added to tables 3-3, 3-4 and 3-5. Does this also apply to
the minimum wrap thickness? (Example) Is it required for a
non-conductive filled through via to have .944 mils of wrap (table 3-3)?
It's a bit confusing as it says to apply to minimum copper average and
minimum thin areas.
Wendi
This communication is for use by the intended recipient(s) only and may contain information that is privileged, confidential, proprietary and exempt from disclosure under applicable law. You are hereby notified that any dissemination, distribution, forwarding or copying hereof is strictly prohibited without the express written consent of DDi. If you have received this communication in error or are not the intended recipient, you should destroy the message and any attachments or copies, and you are prohibited from retaining, distributing, disclosing, or using any information contained herein. Please inform us of the erroneous delivery by return e-mail. Thank you for your cooperation.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|